@Article{, title={Preparation and Characterization of ZnO Nanocrystalline for Photovoltaic Applications Using Laser Ablation Technique}, author={Odai N. Salman and Ibrahim R. Agool}, journal={Al-Nahrain Journal of Science مجلة النهرين للعلوم}, volume={19}, number={2}, pages={87-94}, year={2016}, abstract={The synthesis of ZnO nanocrystalline by laser ablation of a pure zinc metal target in pure water are presented hear. X-ray diffraction (XRD) analysis show that the ZnO nanoparticle is having crystalline wurtzite phase. Transmission electron microscopy (TEM) image illustrate that the ZnO nanoparticles is spherical shape with an average size of about 37 nm. Williamson-Hall (W-H) plot was employed to estimate the crystalline sizes and lattice strain. The optical energy gap were obtained from UV-Vis spectroscopy agreement with that obtained from Photoluminescence spectra. The blue emission were observed when excited the suspension with 335 nm. Dye-Sensitized Solar Cell (DSSC) was successfully fabricated from ZnO nanoparticle using electrostatic deposition technique.

تم تحضير اوكسيد الزنك ذو البنية البلورية والحجم النانوي باستخدام طريقة القلع الليزري لمعدن الزنك النقي المغمور في ماء عالي النقاوة. تحليل الاشعة السينية اظهر ان الجسيمات النانوية لاوكسيد الزنك تمتلك بنية بلورية من الطور wurtzite. ان صورة المجهر الالكتروني النافذ تظهر ان معدل حجم الجسيمات النانوية هو بحدود (37 نانوميتر). ان مخطط ويلمسون- هول وُظِّفَ لحساب الاحجام البلورية وإجهاد الشبيكة. فجوة الطاقة البصرية المحسوبة من طيف الاشعة فوق البنفسجية – المرئية تتفق مع فجوة الطاقة المحسوبة من طيف التلألؤ الضوئي، الانبعاث الازرق تم رصده عندما هيجت العينة ضوئيا بضوء ذو طول موجي (335 نانوميتر) . تم تصنيع خلية شمسية صبغية بنجاح من غشاء اوكسيد الزنك النانوي المرسب باستخدام تقنية الترسيب الكهروستاتيكي.} }