TY - JOUR ID - TI - Corrosion of Carbon Steel Pipeline in Flow System of waterSweetening Plant تأكل أنابيب الصلب الكربوني في منظومة الجريان لمحطة تحليه المياه AU - Mr. Fadhil S. Kadhim فاضل سرحان كاظم AU - Mohammed A. Atiya محمد عبد عطية السراج PY - 2008 VL - 4 IS - 1 SP - 1 EP - 7 JO - Al-Khwarizmi Engineering Journal مجلة الخوارزمي الهندسية SN - 18181171 23120789 AB - The electrochemical behavior of carbon steel in water sweetening station in Libya has been studied in the range of ( 293–333 oC) using weight loss technique. Measurements were carried out over a range of Reynolds number (5000 – 25000).An apparatus was designed for studying the corrosion process in the turbulent regime, which is of industrial significance. It was found that The corrosion rate of carbon steel in water sweetening station is under diffusion control and increases with increasing Reynolds number. On the other hand the variation of corrosion rate with temperature in the range of (293–333 oC) was found to follow Arrhenius equation and the activation energy approximately the same except at low Reynolds number.

تم دراسة السلوك الكهروكيمياوي لمعدن الكربون ستيل في المحلول المائي في محطة التحلية في درنة / ليبيا, حيث تم دراسة تأثير درجة الحرارة وللمدى (293 – 333 ) درجة كلفن , ومديات رقم رينولدز (الجريان) من (5000 – 25000) , باستخدام تقنية الفقدان بالوزن. ولغرض انجاز هذه الدرسة تم تصميم منظومة تعمل تحت ظروف الجريان المضطرب وهو الظرف العملي في محطة التحلية.من خلال الدراسة تبين إن عملية التآكل تحت سيطرة عملية الانتشار Diffusion Control , هذا من جانب ومن جانب آخر فأن معدل التآكل يزداد بزيادة كل من درجة الحرارة والجريان(رقم رينولدز),بالإضافة إلى ذلك لوحظ انطباق معادلة ارهينوس على القيم العملية وبتغير طفيف بأرقام رينولدز المنخفضة. ER -