TY - JOUR ID - TI - Copper Recovery from Spent Etchant Cupric Chloride Solution by Electrowinning Method AU - Zuhaira N. Hanna AU - Aprael S. Yaro PY - 2007 VL - 13 IS - 2 SP - 1344 EP - 1353 JO - Journal of Engineering مجلة الهندسة SN - 17264073 25203339 AB - Recovery of copper from actual spent etchant cupric chloride solution used in manufacturing of printed circuit board (PCB) containing 124 g/l Cu^+2 ions concentration and 60 g/l hydrochloric acid was investigated in a batch mode jacketed tank. This tank was constructed with inner dimensions of 19×10×15 cm^3. Cylindrical rode-shape titanium was used as cathode, while two rectangular shaped graphite were used as anodes. The parameters studied were: current density (0.16-0.30 A/cm^2), copper concentration in etchant solution (30-124 g/l) and the temperature (25-45 °C). The highest current efficiency obtained was about 92% and the lowest power consumption achieved was about 2.7 W.h/g within the temperature range 25-35 °C.

يهدف البحث الى استعادة النحاس بطريقة الترسيب الالكتروليتي من محلول كلوريد النحاس الفائض (المتخلف) من انتاج البطاقات الالكترونية، يحتوي المحلول على ايونات النحاس بتركيز 124 غملتر و حامض الهيدروكلوريك بتركيز 60 غماتر. تم البحث باستخدام نظام الوجبات في خزان ذو جاكيت لغرض التبريد و بابعاد داخلية 19×10×15 سم^3. استخدم قطب كاثود اسطواني الشكل من التيتانيوم و قطبي الانود مستطيلي الشكل من مادة الكرافيت. درست الظروف التشغيلية التالية: كثافة تيار (0.16-0.30 امبيرسم^2) و تركيز ايونات النحاس بالمحلول (31-124 غملتر) و درجة الحرارة (25-45 5^م). اعلى كفاءة تيار تم الحصول عليها كانت حوالي 92 % و اقل طاقة مستهلكة لترسيب النحاس على سطح الكاثود بالساعة كانت حوالي 2.7 واطزساعةغم ضمن درجة الحرارة 25-35 5^م. ER -