TY - JOUR ID - TI - A study of the Hardness and Wear Rate of Elastomer Composites Reinforced by Al2O3 and SiO2 Particles دراسة الصلادة و معدل البلى لمتراكب مطاطي مقوى بدقائق من SiO3 و 2 Al2O AU - Mayyadah Sh. Abed AU - Mohammed S. Hamza AU - Jawad K.Oleiwi PY - 2009 VL - 27 IS - 7 SP - 1422 EP - 1434 JO - Engineering and Technology Journal مجلة الهندسة والتكنولوجيا SN - 16816900 24120758 AB - This research deals with the study the effect of adding the silica particles andalumina particles separately with different ratio (5, 10, 15, 20, and 25 pphr) on thehardness and wear rate of natural rubber NR and styrene butadiene rubber SBR. Theresults show that the hardness increases with the increase the loading level of reinforcingparticles, while the wear rate decreases with the increase the loading level of thereinforcing particles. The largest value of the hardness and the lowest value of the wearrate were for styrene butadiene reinforced with 25 pphr of silica as compared withnatural rubber. Also the reinforcing by SiO2 increases the hardness and decreases thewear rate more than of Al2O3.The results indicated that the hardness and the wear rate for SBR and NRreinforced by SiO2 and Al2O3 at (25 pphr) illustrated in the following table:

تناول هذا البحث دراسة تاثير اضافة دقائق السليكا و الالومين ا بصورة منفصلة و بنسب مختلفة5) على الصلادة و معدل البلى للمطاط الطبيعي و مطاط الستايرين - , 10, 15, 20, and 25 pphr)بيوتادايين. بينت النتائج بان الصلادة تزداد مع زيادة نسب اضافة مادة التقوية , بينما معدل البلى يقل معزيادة نسب اضافة مادة التقوية . حيث ان اعلى قيم للصلادة و اقل معدل بلى تم الحصول عليه هما25 ) مقارنة بالمطاط الطبيعي . pphr) للمطاط الستايرين- بيوتادايين المقوى بدقائق السليكا بنسبةوكذلك عند التقوية بدقائق السليك ا يقل معدل البلى اكثر مم ا عليه عند التقوية بدقائق الالومين ا. حيثالمقوى بدقائق السليكا و الالومينا بنسبة SBR و المطاط NR بلغت قيم الصلادة و معدل البلى للمطاط25 ) موضحة بالجدول التالي: pphr) ER -