TY - JOUR ID - TI - Study of the Thermal Durability of Refractory Mortar Prepared from Local Clay Mixed with Different Percentage of Silica دراسة قوة التحمل الحراري للاسمنت الناري المحضر من الاطيان المحلية والمخلوط مع نسب مئوية مختلفة من السليكا AU - Mustafa Kadhum مصطفى كاظم AU - H.A.Jaffer حارث ابراهيم جعفر PY - 2013 VL - 54 IS - 5 SP - 1096 EP - 1101 JO - Iraqi Journal of Science المجلة العراقية للعلوم SN - 00672904 23121637 AB - Refractory mortar was prepared from the mixing of locally fire clay with different percentage of silica powder (30,40,50,60)wt% by using Pyrometric Cone Equivalent PCE . According to the U.S. Standard ASTM C24, the samples were prepared by using Hand – molding method and dried at temperature 110⁰C and finally firing at different temperature (1000,1100,1200,1300)⁰C according to burning program to study the effect of temperatures for these specimens on the thermal durability .It was shown that the increasing in the percentage of silica content increased the durability of heat specimens, and the best degree of burn was 1300°C.

الاسمنت الناري الذي تم تحضيره من خلال استخدام اطيان حرارية متوفرة محليا وتم خلطه مع نسب مؤية مختلفة من السليكا % ( 30,40,50,60) من خلال استخدام طريقة التحمل الحراري للحراريات وحسب المواصفة الامريكية (24 CASTM ) وقد استخدمت طريقة القولبة اليدوية لتحضير النماذج وبعدها تم تجفيفها في درجة حرارة (110°م) واخيرا حرقت بدرجات حرارة مختلفة (1000,1100,1200,1300°م) وحسب برنامج حرق معين لحساب قابلية تحملها الحراري في هذه الدرجات وقد اظهرت النتائج ان زيادة نسبة السليكا في الاسمنت الناري تزيد من قابليتها لتحمل درجات الحرارة, وان افضل درجة حرارة حرق كانت 1300°م. ER -