TY - JOUR ID - TI - Enhanced of the Two photon Absorption in Nanostructure Wide Band gap Semiconductor CdS using femtosecond Laser تحسين عملية الامتصاص الفوتوني الثنائي في التراكيب النانويه للاشباه الموصلات ذات فجوة الطاقة الواسعة للـ CdS باستخدام ليزر نبضي ذات النبضات الفمتو ثانية AU - Raied K. Jamal رائد كامل جمال AU - Kadhim A. Adem كاظم عبد الواحد AU - Mohammed A. Hameed محمد عبد الله حميد PY - 2014 VL - 5 IS - 1 SP - 65 EP - 70 JO - University of Thi-Qar Journal of Science مجلة علوم ذي قار SN - 19918690 27090256 AB - We observed strong nonlinear absorption in the CdS nanoparticles of dimension in the range 50-100 nm when irradiant with femtosecond pulsed laser at 800 nm and 120 GW/cm2 irradiance intensity. The repetition rate and average power were 250 kHz and 30 mW. The CdS nanoparticles sizes were controlled by reaction time of S-olylamine and Cd-alylamine components interacting at 300 oC. The structures of the prepared CdS nanoparticles was tested and its optical properties were investigated. The nonlinear absorption coefficient was measured using a fully computerized z-scan unit. The results show the value of ß is in order of 116 cm/GW. This value is in a good agreement with values mentioned by other studies.

تم ملاحظة الامتصاص اللاخطي القوي في رقيقة CdS ذات الجسيمات النانوية الابعاد وضمن مدى 50-100 nm عند تشعيعها بنبضات أشعة ليزر تتميز بأمد نبضة بوحدات فيمتوثانية وطول موجي nm800 نانومتر وقدرة اشعاع 120 GW/cm2 . معدل التكرار والقدرة لليزر المستخدم هما 250 kHz و 30 mW على التوالي. ان حجوم الجسيمات النانوية للـ CdS تم السيطرة عليها خلال زمن التفاعل بين المركبين S-olylamine و Cd-alylamine وعند درجة حرارة .300 oC اختبرت الخصائص البصرية للتراكيب الجسيمية النانوية المكونة للرقيقة النانوية CdS وقيس معامل الامتصاص اللاخطي بوحدة z-scan المسيطر عليها كليا بواسطة الحاسوب. بينت النتائج بان قيمة معامل الامتصاص اللاخطي مساوية للـ (116 cm/GW) وهذه القيمة هي عالية مقارنة مع بقية الدراسات حول الموضوع نفسه. ER -