research centers


Search results: Found 2

Listing 1 - 2 of 2
Sort by

Article
Study of Wear Sliding For Dezincification of Brass
دراسة البلى الانزلاقي لعينات البراص المزالة الزنك

Authors: محمد سعيد وحيد --- هناء عرير سميج
Journal: Engineering and Technology Journal مجلة الهندسة والتكنولوجيا ISSN: 16816900 24120758 Year: 2009 Volume: 27 Issue: 14 Pages: 484-499
Publisher: University of Technology الجامعة التكنولوجية

Loading...
Loading...
Abstract

Given the emergence of cracks in a high proportion of clay product in the production phase of the plant Blocks in the laboratory Abu- Nuass which was reflected in the increase of damage from the permissible limits, as well as the high proportion of soluble salts that are on theexternal surfaces of the product, which negatively affect the properties of bricks in the future lead to the break in the walls and turned into a fragile strength, which affects the safety anddurability of origin and to address these negative phenomena and to identify causes and improve the properties of brick products to be within the specification has been adopted for this researchand to take practical steps in the development of a scientific program for the follow-up stages of the process of production and make the appropriate adjustments to it, starting with the initial article and the semi-final and ending with the product. The focus was on developing a program to modify the conditions of drying and burning and theadoption of the drying period of time not exceeding 72 hours and a gradual manner to control on the stresses generated by the sudden evaporation of water. As well as kaolin’s clay been added to the soil and in different proportions were different burning temperature was reached by adding the best results (30-40)% of kaolin’s clay degree burn (950-1000) m into the soil and following the step-by-step method of drying, where it was observed a significant improvement in the properties of bricks in terms of strength and absorption of water and effloresce phenomenon.

70 ) بتأثير الأوساط الأكالة / تضمن البحث دراسة عملية إزالة الزنك التي تحدث في سبيكة براص-الفا ( 30 2,1.5,1,0.5 )ولفترة غمر( 14 ) يوما,وقد كان اقل معدل M) (الحامضية والقاعدية والملحية) عند تراكيز مختلفة 3.37,90.14 ) للأوساط الأكالة الثلاثة الحامضية,القاعدية والملحية ppm)(0.5 M) لحدوث الإزالة عند التركيز 13.29,220,69 ) للأوساط الثلاثة. تم ppm)(2 M) على التوالي.أما أقصى معدل للإزالة فقد كان عند التركيز تعزيز النتائج أعلاه بفحص الخشونة السطحية للعينات التي عوملت بالأوساط أعلاه وللتراكيز نفسها.ولدراسة اثر الإزالة للزنك على خواص سبيكة البراص,تم دراسة تأثير الإزالة في خواص البلى الالتصاقي الجاف تحت تأثير أحمال وسرع مختلفة, وتبين من نتائج الفحص إن العينات المغمورة في الوسط القاعدي اقل مقاومة للبلى. أما العينات المغمورة في الوسط الملحي فأبدت مقاومة بلى أعلى من الوسط القاعدي في حين كانت أعلى مقاومة للبلى للعينات المعاملة بالحامض, ولكن تبقى مقاومة البلى للسبيكة الأصلية أعلى مما في حالة العينات التي تممعاملتها بالأوساط الأكالة.


Article
EFFECT OF H2SO4 ACID ON FATIGUE FAILURE PROPERTY FOR POLYMER MATRIX COMPOSITE
تأثير حامض الكبريتيك على خاصية الكلال لمتراكبات الايبوكسي

Loading...
Loading...
Abstract

:This research include the study of the fatigue property for the polymer and the composite materials, we using the epoxy resin as matrix for the reinforced materials that consist of artificial fibers (Kevlar, glass and PVC fibers) also aluminum powder for reinforcing.
The slates made of composite materials and hybrid composite materials for both volume fractions30% and 40% from the reinforced materials, where we made twenty one slates from the composite materials, all these slates cutting to samples with measurement (10x 70mm) in order to execute the fatigue test accordingly for the fatigue machine characteristics, these samples divided to several groups for both volume fractions 30% and 40%, these groups immersing in H2SO4 acid for fifty day to study the effect of this solution in the fatigue characteristic.
The test executed by two steps: - the first step include executing the fatigue testing for the dry samples and comparison these results with each other, the second step include the fatigue test for the samples after immersion in the solution (H2SO4 acid) for fifty day,. The results of fatigue test from the second step comparing with the results from the first group for both volume fractions 30% and 40%. The results and laboratory examinations for these samples show a decreasing in the number of fatigue cycles until the fail when the applied load or applied stress increase

تضمن البحث دراسة خاصية الكلال للمواد المتراكبة البوليمرية ، حيث استخدم راتنج الايبوكسي كمادة رابطة لموادوكذلك تتضمن مسحوق الالمنيوم (PVC التدعيم والتي تتكون من الالياف الصناعية (الياف الكفلر والزجاج ولغرض التدعيم ايضا.صنعت الواح من المواد المتراكبة والمواد المتراكبة الهجينة وبالكسرين الحجميين % 30 و % 40 من مواد(10x70mm) التسليح ، حيث تم تصنيع ( ٢١ ) لوحا من هذه المواد. هذه الالواح قطعت الى عينات بالقياساتلكي يتم فحص الكلال لها وتبعا لمواصفات الجهاز المستخدم ، هذه العينات قسمت الى عدة مجاميع لكلا الكسرين1) لمدة خمسون يوما لدراسة تأثير N) الحجميين ومن ثم غمرت في محلول حامض الكبريتيك المخفف ذي التركيزهذا الحامض على خاصية الكلال للمواد المتراكبة .اجري فحص الكلال بمرحلتين :- المرحلة الاولى اجراء فحص الكلال للعينات وهي جافة ومن ثم مقارنة نتائجالفحص فيما بينها . اما المرحلة الثانية فقد نفذ فحص الكلال للعينات بعد غمرها بالمحلول الحامضي لمدة خمسونيوما وقد تم مقارنة النتائج الحاصل عليها في هذه المرحلة مع نتائج المرحلة الاولى ولكلا الكسرين الحجميين منالتسليح . اظهرت النتائج والفحوصات المختبرية للعينات ان هناك تناقصا في عدد الدورات الى حد الكلال عند زيادةالحمل او الاجهاد المسلط عليها .