The Effect of Elevated Temperature of Compressive Strength of Steel Fiber Concrete

Author: Osama M. Ghazi
Journal: Journal of University of Babylon مجلة جامعة بابل ISSN: 19920652 23128135 Year: 2013 Volume: 21 Issue: 3 Pages: 1006-1012
Publisher: Babylon University جامعة بابل

Loading...
Loading...
Abstract

This study presents the benefit gained from using steel fiber reinforcement on concrete mixture. The effect of fire on compressive strength is investigated. Two different tests, one of them is the non destructive test which is the ultrasonic pulse velocity (UPV) test and the other is the destructive compression test, are carried out using (10cm) cubes. Forty-eight cubes (half of them are with steel fiber reinforcement of fiber/concrete ratio of (0.01) by volume and the remaining cubes are without fiber reinforcement) are heated to temperature levels of (100,200,300,400,500,600 and 700°C). Then after that specimens are air cooled and (UPV) test is done, the specimens are destructively tested. The results indicated that the addition of steel fiber increases the compressive strength at all tested heating levels with a maximum percentage increase of (56.9%) at a temperature level of (500°C), in spite of that they have the same behavior but the residual compressive strength decreases with the addition of steel fiber for the tested heating levels lower than (400°C) and increases for the heating levels above this degree

الدراسة الحالية تسلط الضوء على الفائدة الحاصلة من تسليح الألياف الفولاذية في تكنولوجيا الخرسانة حيث بحث تاثير الحرارة على مقاومة انضغاطها.اجري نوعان من الفحص احدهما لااتلافي وهو فحص سرعة الأمواج فوق الصوتية (UPV)والأخر إتلافي باستعمال نماذج مكعبة بطول ضلع(10سم).تم تسخين(48) نموذج (نصفها مقواة بألياف الفولاذ بنسبة حجمية للالياف الفولاذية إلى الخرسانة مقدارها(0.01)والنماذج الأخرى المتبقية غير مقواة) إلى مستويات من درجات الحرارة هي(100و200و300و400و500و600و700)درجة سيليزية.فحصت النماذج لا اتلافيا بعد تبريدها بتعريضها للهواء ثم فحصت اتلافيا.بينت النتائج ان إضافة الألياف الفولاذية يزيد من مقاومة الانضغاط في كل مستويات درجات الحرارة التي قيست فيها باعلى نسبة زيادة مقدارها (56.9%) من تلك غير المقواة عند درجة حرارة (500) درجة سيليزية بالرغم من ان لهما نفس السلوك ولكن نسبة ما تبقى من المقاومة بعد الحرق من المقاومة الاصلية يقل باضافة الالياف الفولاذية عند كل مستويات درجات الحرارة الأقل من (400)درجة سيليزية ولكنها تزداد بعد تلك الدرجة.


Article
Experimental Study for Punching Shear Behavior in RC Flat Plate with Hybrid High Strength Concrete
دراسة عملية لمقاومة القص الثاقب للسقوف الخرسانية المستوية المصنوعة من الخرسانة الهجينية عالية الانضغاط

Authors: Ban Sahib A. بان صاحب --- Shatha S. Kareem شذى صاحب كريم --- Ali H. Aziz علي حميد عزيز
Journal: Journal of Engineering and Sustainable Development مجلة الهندسة والتنمية المستدامة ISSN: 25200917 Year: 2013 Volume: 17 Issue: 3 Pages: 105-119
Publisher: Al-Mustansyriah University الجامعة المستنصرية

Loading...
Loading...
Abstract

This Paper is conducted to investigate experimentally the punching shear behavior of hybrid flat plate. Five slab specimens with (1000x1000x70) mm dimensions have been tested, two of which have been made fully with High Strength Concrete and Steel Fiber Reinforced Concreter , while, the others have been made by mixing two types of concrete (Steel Fiber Reinforced Concreter in the critical zone and High Strength Concrete in the other part of slab specimen). The slab dimensions, main reinforcement have been kept constant in all slab specimens. The variables are concrete type and dimensions of critical area. Experimental results show that the use of SFRC improves the punching shear resistance and allows higher forces to be transferred through the slab-column connection. For slab specimen which made fully with SFRC, the ultimate shear capacity increased by (25%) in comparison with the normal slab. While, for slab specimens which made with hybrid concrete the ultimate shear capacity increased by (5%-13%) in comparison with the normal slab.

تأثير استخدام أنواع مختلفة من الخرسانة (الخرسانة الهجينية) في المنطقة الحرجة لالتقاء العمود مع البلاطة على مقاومة القص الثاقب في البلاطات الخرسانة الصفائحية تمت دراستها في هذا البحث. تم فحص خمسة بلاطات مربعة الشكل بأبعاد (1000*1000*70) ملم بالإضافة الى سلسلة من الفحوصات التي تم أجراءها على نماذج السيطرة لدراسة الخواص الميكانيكية لأنواع الخرسانة المستخدمة. المتغيرات في هذه الدراسة هي نوع الخرسانة في المنطقة الحرجة وأبعاد هذه المنطقة مع الإبقاء على أبعاد البلاطات و حديد التسليح دون تغيير .تعرضت كلا من النماذج المرجعية و بلاطات الفحص الى نفس الظروف المختبرية. أظهرت النتائج المختبرية أن الزيادة في مقاومة انضغاط الخرسانة حسن مقاومة القص الثاقب وهذا يسمح بانتقال قوة اكبر من خلال المفصل الرابط بين العمود والبلاطة. كذلك، بينت النتائج أن مقاومة القص الثاقب قد ازدادت بمقدار (25%) بالنسبة للبلاطات المسلحة بالكامل بألياف الحديد عند مقارنتها مع البلاطة العادية. أظهرت النتائج، كذلك، حصول زيادة في المقاومة القصوى للقص الثاقب بمقدار (5%-13%) بالنسبة للبلاطات المسلحة جزئيا بألياف الحديد عند مقارنتها مع البلاطة العادية.