research centers


Search results: Found 8

Listing 1 - 8 of 8
Sort by

Article
MANUFACTURING AND NUMERICAL ANALYSIS OF ELBOW ORTHOSIS MADE OF POLYPROPYLENE – CARBON FIBER – POLYPROPYLENE

Author: Sameer Hashim Ameen
Journal: Journal of Engineering and Sustainable Development مجلة الهندسة والتنمية المستدامة ISSN: 25200917 Year: 2016 Volume: 20 Issue: 4 Pages: 186-199
Publisher: Al-Mustansyriah University الجامعة المستنصرية

Loading...
Loading...
Abstract

In this work, elbow orthosis which represents one of the upper extremity orthosis is manufactured from two layers of polypropylene reinforced by a sheet of carbon fiber between them to construct a new composite material called "PCP" material. More flexibility is gained by minimization of the modulus of elasticity of polypropylene-carbon fiber- polypropylene to about 3.5 against old material. Average pressure is measured between the patient's arm and bicep part of elbow using a portable pressure device (has mat of sensors) which reach to about 217 kPa. ANSYS PACKAGE version 11 is used for numerical analysis the bicep part of elbow by using the estimated internal pressure to investigate deformation and to determine the Von – Misses stress. The investigated numerical results showed that the new material maximizes the deformation to about 280 % ( still in elastic region) and make the design more safe by increasing the factor of safety more than 4 % against polypropylene material. Mechanical properties are measured also in present work by carrying out the tensile test for the two materials under study to conclude finally that, the sheet of carbon fiber which is added has increased the mechanical properties to about 8.25 % and 248 % for yield and ultimate stresses respectively.

في هذا البحث, تم تصنيع مسند كوع والذي يمثل احد انواع المساند العلوية من طبقتين من مادة البولي بروبلين مع شريحةكاربون محشوة بينهما لغرض تشكيل مادة مركبة جديدة تدعى ) PCP (. نحصل على مرونة اكثر بتقليل معامل المرونة للمادة المركبة بوليبروبلين شريحة كاربون بولي بروبلين لغاية معامل – – 3.5 من المادة القديمة. تم قياس معدل الضغط المتولد بين الذراع العلوي للمريضومسند الكوع باستخدام جهاز ضغط محمول ) يمتلك حصيرة من المتحسسات( ليصل الى 217 كيلوباسكال. استخدم برنامج ANSYSللنسخة 11 للتحليل العددي للجزء العلوي للمسند من خلال تطبيق الضغط المقاس سلفا وذلك لايجاد اجهاد فون مايسز. اظهرت النتائجالمستحصلة عدديا زيادة للتشوة للمادة الجديدة بمقدار 280 % عن المادة القديمة ) ولا تزال ضمن منطقة المرونة ( وكذلك جعل التصميماكثر امانا من خلال زيادة معامل الامان بحدود 4 %. في البحث الحالي تم قياس الخصائص الميكانيكية عن طريق اجراء اختبار الشد لكلاالمادتين موضوع البحث واستنتج ان اضافة شريحة الكاربون عملت على زيادة اجهاد الخضوع والاجهاد الاقصى بمقدار 8.25 % و 248% على التوالي.


Article
Evaluation of the Effect of silanized Zirconium Oxide nano-fillers and Plasma Treated polypropylene fibers Addition on some Properties of Heat Cured Acrylic Resin Denture Base Material

Author: Dr. Noor Falah Abdul-Hadi, B.D.S., M.Sc. * د.نور فلاح عبدالهادي
Journal: MUSTANSIRIA DENTAL JOURNAL مجلة المستنصرية لطب الاسنان ISSN: 18138500 Year: 2016 Volume: 13 Issue: 1 Pages: 70-76
Publisher: Al-Mustansyriah University الجامعة المستنصرية

Loading...
Loading...
Abstract

Background: The polymethylmethacrylate is the most reliable material for theconstruction of dentures but it has the disadvantages of lacking strength andradio-opacity. The purpose of this study was to evaluate the effect of addition ofmodified nano-zirconium oxide (zro2 ) and plasma treated polypropylene fiberson some mechanical properties of heat cure acrylic resin materials.Materials and methods:- Zirconium oxide nanoparticles were coated with a layer ofpropyltrioxysilane before dispersed and sonicated in monomer(MMA)inpercentage of 2% by weight . The plasma treated polypropylene fibers were inpercentage of 2% by weight added to polymer powder. Sixty specimens wereconstructed and divided into 3 groups according to the using tests; each groupwas subdivided into two subgroups. The tests used were impact strength,transverse strength and surface hardness. Data were analyzed T-test.Results:- After the addition of plasma treated polypropylene fibers and modifiednano-Zro2 fillers there was a highly significant increase in impact strength,transverse strength and surface hardness.Conclusion: It can be concluded that the addition of modified nano-Zro2 fillers andplasma treated polypropylene fibers effective method to enhance the fractureresistance of acrylic denture base material.


Article
Evaluation the Effect of Addition of Plasma Treated Polypropylene Fiber and Silanized Silicon Dioxide Nanoparticles Composite on Some Properties of Heat-Polymerized Polymethylmethacrylate

Authors: Ahmed G. Ahmed احمد غيث احمد --- Intisar J. Ismail انتصار جميل اسماعيل
Journal: Journal of baghdad college of dentistry مجلة كلية طب الاسنان بغداد ISSN: 16800087 Year: 2016 Volume: 28 Issue: 4 Pages: 1-8
Publisher: Baghdad University جامعة بغداد

Loading...
Loading...
Abstract

Background: Polymethylmethacrylate (PMMA) is the most commonly used material in denture construction. This material is far from ideal in fulfilling the mechanical requirements, like low impact and transverse strength and poor thermal conductivity are present in this material.The purpose of this study was to study the effect of addition a composite which include 1%wt silanized silicone dioxide nano fillers (SiO2) and 1wt% oxygen plasma treated polypropylene fiber (PP) on some properties of heat cured acrylic resin denture base material (PMMA).Materials and methods: One hundred (100) prepared specimens were divided into five groups according to the tests, each group consisted of 20 specimens and these were subdivided into two groups (unreinforced heat cured acrylic resin as control group)and reinforced acrylic resin with ( 1%wt Nano SiO2 and 1% wt oxygen plasma treated polypropylene fibers) group. The transverse strength¸ impact strength, indentation hardness (shoreD), surface roughness and water sorption and solubility were investigated. The results were statistically analyzed using descriptive and t-test.Results: The results of this study show that a highly significant increase in impact strength (10.4939 Kj/m2),surface hardness (89.9375) surface roughness (0.9498) and water sorption (0.0171mg/cm2) was observed with the addition of 1%wt silanized (SiO2) nanoparticles and 1%wt oxygen plasma treated polypropylene fibers to (PMMA) , also significant decrease in transverse strength (103.4753 N/mm2), nonsignificant decrease occurred in water solubility which was (0.0005mg/cm2).Conclusion: The incorporation of 1%wt silanized SiO2 nanoparticles and 1%wt oxygen plasma treated polypropylene fiber to heat cure PMMA form a composite improves the impact strength, surface hardness and surface roughness of acrylic resin, at the same time this addition increase the water sorption and decrease water solubility; while significant decrease in transverse strength


Article
EVALUATION OF MECHANICAL PROPERTIES OF HIGH PERFORMANCE SELF-CONSOLIDATED CONCRETE ENHANCED BY DISCRETE STEEL AND POLYPROPYLENE FIBERS
تقييم الخواص الميكانيكية للخرسانة عالية الأداء الذاتية الرص المعززة بالألياف الحديدية المنفصلة وألياف البولي بروبلين

Author: Ali Adel Abdulhameed
Journal: Journal of Engineering and Sustainable Development مجلة الهندسة والتنمية المستدامة ISSN: 25200917 Year: 2016 Volume: 20 Issue: 4 Pages: 34-52
Publisher: Al-Mustansyriah University الجامعة المستنصرية

Loading...
Loading...
Abstract

High performance self-consolidating concrete HP-SCC is one of the most complex types of concrete which have the capacity to consolidated under its own weight, have excellent homogeneity and high durability. This study aims to focus on the possibility of using industrial by-products like Silica fumes SF in the preparation of HP-SCC enhanced with discrete steel fibers (DSF) and monofilament polypropylene fibers (PPF). From experimental results, it was found that using DSF with volume fraction of 0.50 %; a highly improvements were gained in the mechanical properties of HP-SCC. The compressive strength, splitting tensile strength, flexural strength and elastic modulus improved about 65.7 %, 70.5 %, 41.7 % and 80.3 % at 28 days age, respectively with retaining the main properties of HP-SCC. Furthermore, using PPF with volume fraction up to 0.10 %; an enhancement in the compressive and elastic modulus of HP-SCC about 47.4 % and 31 % was obtained at age of 28 days, respectively. Moreover, using PPF with volume fraction of 0.15 %, the splitting tensile strength and flexural strength of HP-SCC improved about 44.5 % and 20.3 %, respectively.

تعتبر الخرسانة العالية الأداء والذاتية الرص واحدة من أعقد أنواع الخرسانة التي لها القابلية على الرص تحت تأثير وزنها الذاتي فضلاً عن تجانسها الممتاز وديمومتها العالية. هذه الدراسة العملية تهدف إلى إستخدام أبخرة السليكا كمنتج صناعي ثانوي في إنتاج الخرسانة عالية الأداء والذاتية الرص والمعززة بألياف حديدية منفصلة وألياف البولي بروبلين أحادية الشعيرة. بينت نتائج الفحوصات العملية، إن أستخدام الألياف الحديدية المنفصلة بنسبة 0.5 % من حجم الخرسانة أدى إلى تحسن عالي في الخواص الميكانيكية لها حيث زادت كل من مقاومة الأنضغاط ، مقاومة إنفلاق الشد، مقاومة الإنثناء و معامل المرونة بنسبة 65.7 % ، 70.5 % ، 41.7 % ، 80.3 % وعلى الترتيب لمعدل النماذج الخرسانية المختلفة وبعمر 28 يوماً. علاوة على ذلك، إن أستخدام ألياف البولي بروبلين أحادية الشعيرة بنسبة لاتتجاوز 0.10 % من حجم الخرسانة أدى إلى زيادة مقاومة الأنضغاط ومعامل المرونة للخرسانة عالية الأداء والذاتية الرص بنسبة 47.4 % ، 31 % بعمر 28 يوماً، على الترتيب. أيضاً، إن أستخدام الألياف الأخيرة بنسبة حجمية مقدارها 0.15 % أدى إلى تحسن مقاومة إنفلاق الشد ومقاومة الإنثناء للخرسانة وبعمر 28 يوماً لمعدل النماذج الخرسانية المختلفة بنسبة 44.5 % ، 20.3 %، على الترتيب.


Article
Effect of Steel Fibers, Polypropylene Fibers and/ or Nanosilica on Mechanical Properties of Self-Consolidating Concrete
تأثير الالياف الفولاذية والياف البولي بروبلين مع او بدون الحبيبات النانوية السليكية على الخواص الميكانيكية للخرسانة الذاتية الرص

Authors: Iqbal N. Gorgis --- Maan S. Hassan --- Rana T. Abdulkareem
Journal: Engineering and Technology Journal مجلة الهندسة والتكنولوجيا ISSN: 16816900 24120758 Year: 2016 Volume: 34 Issue: 3 Part (A) Engineering Pages: 527-538
Publisher: University of Technology الجامعة التكنولوجية

Loading...
Loading...
Abstract

This research concerned studying the combined effect of using nano-silica and/ or hybrid fibers on key mechanical properties of self-consolidating concrete SCC. A comprehensive experimental work has been carried out, using steel fiber (SF) with volume fraction (0, 0.5% and 1.5%), polypropylene fiber (PPF) (0%, 0.05% and 0.15%) and SiO2 nanoparticles (0%, 2% and 4%) by weight of powdered material (silica fume- Sf ) with constant w/c ratio (0.48) to produce eleven different mixtures and tested at different ages (7, 28 and 90 days). Results showed that adding fibers adversely affect SCC workability and thus more dosage of super plasticizer (SP) should be added to stay within the standard limits. comparable to conventional concretes, the presence of steel fibers with SCC provide slight increase in compressive strength at 28 days, (up to 11%), while significant enhancement in tensile properties were observed (up to 24% and 32% for splitting and flexural strength respectively). Polypropylene or hybrid fibers however, provide lower enhancement compared with steel fibers. In contrast, implementation of nanosilica leads to significant improvement in concrete strengths particularly at 4% dosage. Combined effect of 4% nanosilica and 1.5% of steel fibers provide the superior hardening effect on the flexural performance compared with softening effect provided by other added dosages. Scanning Electron Micrograph (SEM) images confirm the matrix densification effect due to nanosilica adding. Flexural strength of SCCs without nanosilica was generally higher than splitting testing results. This fact does not change even with the presence of nanosilica and/ or fibers.

تم دراسة التاثير المشترك لاستخدام الحبيبات النانوية السليكية مع او بدون الالياف المهجنة على الخواص الميكانيكية للخرسانة ذاتيـــــة الرص. من اجل دراسة هذا التأثير تـــــم القيام بفحوصات مختبرية باستخدام الالياف الفولاذيــــة بنسبـة ( 0 % و 0.5% و1.5% ) والالياف البولي بروبلين بنسبة ( 0% و0.05 % و 0.15.% ) وحببيبات النانو سليكا بنسبة (0% و2% و 4.% ) 2%) كنسبة من وزن المواد الناعمة مع نسبة ثابتة من الماء الى السمنت (0.48) لانتاج احد عشر خلطة مختلفة ومفحوصة بمختلف الاعمار7 و 28 و 90 يوم. النتائج اشارت الى حصول تأثير عكسي عند اضافة الالياف على القابلية التشغيلية الخرسانية لذا تطلب اضافة نسبة اكثر من المضاف الكيميائي الملدن المتفوق للثبات ضمن حدود المواصفات. ان اضافة الالياف الفولاذية الى الخلطة الخرسانة ذاتية الرص ادى الى زيادة قليلة في مقاومة الانضغاط عند عمر28 يوم بمقدار11% بينما زيادة كبيرة في خواص الشد الى حوالي 24%) و(32% لمقاومتي الانشطار والانثناء بالتتابع. اما الالياف البولي بروبلين او الخليط من الالياف يعطي تحسن اقل مما في حالة الالياف الفولاذية. بالمقارنة مع الالياف فان حبيبات SiO2النانوسليكا تؤدي الى تحسن كبير في مقاومة الخرسانة خصوصا عند نسبة اضافة 4%. التأثير المشترك للحبيبات النانوية بنسبة 4% مع الالياف الفولاذية بنسبة 1.5% يعطي تاثير افضل على الخواص الصلبة. بالنسبة لفحص البنية المجهرية فيتوافق مع التأثير المكثف للتراكيب الداخلية للعجينة السمنتية نتيجة استخدام الحبيبات النانوية. كما لوحظ ان مقاومة الانثناء للخرسانة الذاتية الرص بدون المواد النانوية كانت اعلى من نتائج فحص مقاومة الانشطار. لذا هذه الحقيقة لا تتغيربوجود المواد النانوية مع او بدون الالياف.


Article
PROPERTIES OF HIGH STRENGTH LIGHTWEIGHT AGGREGATE CONCRETE PAVING BRICKS
خواص طابوق الرصف من خرسانة الركام خفيف الوزن عالية الاداء

Authors: Suhad Abd Al-Jabbar Mozan --- Wasan Ismail Khalil
Journal: DIYALA JOURNAL OF ENGINEERING SCIENCES مجلة ديالى للعلوم الهندسية ISSN: 19998716/26166909 Year: 2016 Volume: 9 Issue: 3 Pages: 120-132
Publisher: Diyala University جامعة ديالى

Loading...
Loading...
Abstract

This investigation aims to study the properties of paving brick products made from high strength lightweight aggregate concrete (HSLWAC). The mix proportion is 1: 1.35: 0.87 (cement: sand: coarse aggregate) by weight with 520 kg/m3 cement. Local porcelinate coarse aggregate, with maximum size of 9.5 mm, 5% silica fume as partial replacement by weight of cement, 1% by weight of cement superplasticizer, and w/c ratio of 0.29, was used in the mix. Fibers are used including macro hooked steel fiber with aspect ratio 100, micro polypropylene fiber (pp), and micro carbon fiber (CF). Concrete paving brick was produced from three different HSLWAC mixes including, concrete mix without fibers (reference mix), hybrid fibers reinforced concrete mix containing 0.75% volume fraction of steel fiber and 0.25% volume fraction of polypropylene fiber, and hybrid fibers reinforced HSLWAC mix with 0.75% volume fraction of steel fiber and 0.25% volume fraction of carbon fiber. Experimental tests including, compressive strength, absorption, abrasion resistance as well as the appearance were carried out for the produced paving bricks.The results indicated that the produced HSLWAC paving bricks can be classified as medium loading type according to Iraqi Specification No. 1606-2009. This type is used for paving low loaded roads and service areas.

يهدف هذا البحث دراسة خواص طابوق الرصف الخرساني المنتج من خرسانة عالية المقاومة ذات ركام خفيف الوزن وبنسبة خلط وزنية 1.35:1:0.87: ( سمنت: رمل :ركام ) بمحتوى سمنت 520 كغم/م3 سمنت. تم استخدام البورسيلنايت المحلي كركام خشن وبمقاس اقصى 9.5 مم ، 5% ابخرة السليكا المكثفة كأستبدال جزئي من وزن الأسمنت ، 1% من وزن الاسمنت ملدن متفوق و 0.29 نسبة الماء/ الاسمنت . الالياف المستخدمة تضمنت الياف فولاذية طويلة معقوفة النهايات وبنسبة باعية 100، ألياف البولي بروبلين الدقيقة والياف الكاربون الدقيقة . تم انتاج هذا الطابوق من ثلاث خلطات خرسانية عالية المقاومة خفيفة الوزن شملت خلطة خرسانية بدون الياف (الخلطة المرجعية) ، خلطة خرسانية حاوية على 0.75% الياف فولاذية +0.25% الياف البولي بروبلين ، خلطة خرسانية حاوية على 0.75% الياف فولاذية + 0.25% الياف الكاربون . تم اجراء فحوصات مختبرية لطابوق الرصف الخرساني المنتج تضمنت فحص مقاومة الانضغاط ، فحص الامتصاص ، فحص مقاومة البري ،وفحص المظهر. أظهرت النتائج ان الطابوق المنتج يصنف وحسب المواصفة العراقية 1606 كطابوق رصف خرساني من النوع متوسط التحميل والذي يستخدم لرصف الطرق والمناطق الخدمية. الكلمات الدالة: الخرسانة خفيفة الوزن, الهجينة, الالياف, الماكرو, المايكرو, الالياف الفولاذية, الياف الكاربون, الياف البولي بروبلين, طابوق الرصف.


Article
STUDY THE EFFECT OF POLYPROPYLENE FIBERS IN SOME MECHANICAL AND PHYSICAL PROPERTIES OF RIGID POLYURETHANE FOAM COMPOSITES
دراسة تأثير الياف البولي بروبلين في بعض الخواص الميكانيكية والفيزيائية لمادة متراكبة من رغوة البولي يورثان الصلبة

Author: Ismail Ibrahim Marhoon1
Journal: Journal of Engineering and Sustainable Development مجلة الهندسة والتنمية المستدامة ISSN: 25200917 Year: 2016 Volume: 20 Issue: 4 Pages: 71-87
Publisher: Al-Mustansyriah University الجامعة المستنصرية

Loading...
Loading...
Abstract

A foam composite material was set by adding polypropylene fibers diameter of 18 μm and 6 and 12 mm length to rigid polyurethane foam with a weight fraction of (2.5-15 )%wt. The results had shown improvement on (flexural strength, compressive strength, hardness, impact strength) and increase in flexural modulus, density and water absorption, with decreases in thermal conductivity of the resultant foam composite as compared with neat rigid polyurethane foam

مادة رغوية متراكبة تم تصنيعها بواسطة إضافة الياف البولي بروبلين بقطر 18 مايكرون و طول 6 و 12 ملم الى رغوةالبولي يورثان الصلبة بنسب وزنية مئوية (15-2.5) % . اظهرت النتائج تحسناً في) مقاومة الانحناء, مقاومة الانضغاط, الصلادة,مقاومة الصدمة (, وزيادة في معامل الانحناء و الكثافة و امتصاصية الماء مع انخفاض في الموصلية الحرارية للمتراكب الرغوي الناتجعند مقارنته مع رغوة البولي يورثان الصلبة الصرف.


Article
Effect of Silica Fume and Polypropylene Fibers on the Mechanical Properties of Pervious Concrete
تأثير غبار السليكا والياف البولي بروبلين على الخواص الميكانيكية للخرسانة النافذة

Author: Haider Araby Ibrahim
Journal: Muthanna Journal of Engineering and Technology(MJET) مجلة المثنى للهندسة والتكنولوجيا ISSN: 25720317 25720325 Year: 2016 Volume: 4 Issue: 2 Pages: 95-103
Publisher: Al-Muthanna University جامعة المثنى

Loading...
Loading...
Abstract

In this paper, Silica Fume (S.F.) be used for reinforce pozzolanic cement paste and the effect of using many weight percentages as (0%, 5%, 10%, 15%, and 20%) to lessening the concrete weight as a cement replacement in concrete mixtures on the mechanical properties was studied. High range water reducing added to decrease the water demand of the concrete, when silica fume added. Moreover, (0.025%, 0.05%, 0.1%, and 0.15%) are the proportions of polypropylene Fibers (P.P.F.) by volume, which used to improve the pervious concrete mechanical properties, physical, and mechanical properties of hardened concrete containing voids ratio, compression strength, and flexural strength and, splitting tensile strength investigated. The density of reference pervious concrete that was get through the experimental work was( 1835 Kg/m3 ) at (28) days ,it permeability coefficient (K) and voids content was( 0.324) cm/s, and (30.21%) successively, The results shown important increase in compression, splitting tensile and flexural strengths of pervious concrete containing silica fume and (P.P.F.) comparison with reference pervious concrete. The mixture of (10%) of (SF) and (0.1%) of (P.P.F.) gave optimum increased in the compressive, flexural, and splitting tensile strengths compared with the reference mix and the results (47.8%, 29.21%, and 24.41%) respectively.

في هذه البحث، تم أستخدم غبار السليكا لتقوية البوزولانية لعجينة الأسمنت وباستخدام عدة نسب وزنية وهي (0٪، 5٪، 10٪، 15٪، و20٪) من وزن الاسمنت لتقليل الوزن الكلي للخرسانة النافذة من خلال استخدامها كبديل عن الاسمنت وتأثيرها على الخواص الميكانيكية للخلطات الخرسانية النافذة. استخدمت مخفضات المياه عالية المدى لتقليل الطلب على المياه من الخرسانة، عند إضافة غبار السليكا. وعلاوة على ذلك، تم استخدام عدة نسب هي (٪0.025، ٪0.05، 0.1 %، و0.15٪) والتي تمثل نسب ألياف البولي بروبلين الحجمية المستخدمة لتحسين الخواص الميكانيكية للخرسانة النافذة و تم اختبار الخصائص الفيزيائية والميكانيكية للخرسانة النافذة المتصلبة بما في ذلك نسبة الفراغات واختبار النفاذية ومقاومة الانضغاط وقوة الشد الانشطاري ومقاومة الانحناء. بينت النتائج ان كثافة الخرسانة النافذة المرجعية (1835) كغم/ م 3 في (28) يوما، والمحتوى الفراغي ومعامل ال نفاذية كان (0.324) سم / ث، و (٪30) على التوالي، كذلك كانت هناك زيادة كبيرة في مقاومة الانضغاط وقوة الشد الانشطاري ومقاومة الانحناء من الخرسانة النافذة التي تحتوي على غبار السليكا والياف البولي بروبلين مقارنة مع الخلطة المرجعية. خليط من (10٪) من (غبار السليكا) و (0.1٪) من (الياف البولي بروبلين) أعطى أكبر زيادة في مقاومة الانضغاط وقوة الشد الانشطاري ومقاومة الانحناء مقارنة مع الخلطة المرجعية وكانت النتائج (47.8٪، 29.21٪، و24.41٪) على التوالي.

Listing 1 - 8 of 8
Sort by
Narrow your search

Resource type

article (8)


Language

English (8)


Year
From To Submit

2016 (8)