Article
Studying The Bonding Mechanismand Microstructure for Arc Welding of Dissimiler Steel to Copper
البنیة المجھریة وآلیة الربط لملحومات القوس الكھربائي غیر المتماثلة فولاذ الى النحاس

Author: عبد الله عذيب مشاري
Journal: Thi-Qar University Journal for Engineering Sciences مجلة جامعة ذي قار للعلوم الهندسية ISSN: 20759746 Year: 2011 Volume: 2 Issue: 1 Pages: 1-15
Publisher: Thi-Qar University جامعة ذي قار

Loading...
Loading...
Abstract

The aim of this work is to study thebonding mechanism and the microstructure of copper to steel welded by shielded metal arc welding (SMAW). The electrodes that used are ECuSi and ECuSn8thenthe examination of microstructure by optical microscopic, it is clearlyobserved that the copper side are completely interfering with epitaxial growth when using ECuSn8 but the side of steel reveal interaction waves at the interface with nonepitaxial growth. Some of fine cracks observed at the interface with ECuSi. The use of ECuSn8 explaininterfering fine blockes from the steel inside the fusion zone.


Article
Refinement the Microstructure of Al–7Si Alloy by the Addition of Cadmium

Author: Sura Abd Al-Zahrah Muhsion
Journal: Journal of University of Babylon مجلة جامعة بابل ISSN: 19920652 23128135 Year: 2012 Volume: 20 Issue: 1 Pages: 62-66
Publisher: Babylon University جامعة بابل

Loading...
Loading...
Abstract

Cadmium (Cd) modified aluminium–silicon cast alloys are well known for their outstanding mechanical properties as they combine excellent strength with good ductility that is due to a modification of brittle Si in the eutectic with traces of Cd (0.2–1.0 wt%). The results showed that the Cd leads to the refinement of eutectic silicon from ~95 to 10µm. The alloys which used in this work were Al-7Si alloy with additions of 0.2, 0.6 and 1 wt% Cd as well as Al-7%Si with out Cd addition. The effect of keeping time also studied and the results indicate that the addition of 1%Cd with keeping time 3min was the best (about 10 µm).

تكون مصبوبات سبائك الألمنيوم-سليكون، المعدلة بنيتها البلورية بإضافة كميات محسوبة من الكادميوم، ذات خواص ميكانيكية عالية. وهذه الخواص ناتجة عن الجمع بين المتانة العالية والمطيلية الجيدة والناتجة عن تعديل البنية البلورية لطور السليكون الايوتكتيكي من شكل رقائق أو صفائح هشة إلى شكل خيطي منتظم وذلك بفعل إضافة الكادميوم لغاية 1% كمعدل للبنية البلورية. تشير نتائج فحص البنية المجهرية لطور السليكون الايوتكتيكي إلى أن المصبوبة المضاف إليها كادميوم بنسبة 1% قد يصل تحول هذا الطور من شكل ابري أو رقائقي ذو طول حوالي 95 مايكرون إلى خيطي بطول حوالي 10 مايكرون . إن السبائك التي تم دراستها في هذا البحث هي ألمنيوم-7%سليكون بإضافة الكادميوم بنسب(0.2، 0.6 و 1.0%) إضافة إلى السبيكة الأصلية بدون إضافات. كذلك تم دراسة تأثير وقت الحفظ عند درجة حراة إضافة الكادميوم وقد أظهرت النتائج إن المصوبة التي أضيف لها الكادميوم بنسبة 1.0% ووقت حفظ 3 دقائق كانت هي الأفضل (طول السليكون الايوتكتيكي الخيطي10 مايكرون).


Article
EFFECT OF THERMOMECHANICAL TREATMENTS ON AGING BEHAVIOR AND FRACTURE TOUGHNESS OF AL-CU-MG ALLOY PLATES USED IN AIRCRAFT STRUCTURE

Author: Dr. Alaa A. Ateia,
Journal: Iraqi journal of mechanical and material engineering المجلة العراقية للهندسة الميكانيكية وهندسة المواد ISSN: 20761819 Year: 2009 Volume: 9 Issue: 1 Pages: 53-67
Publisher: Babylon University جامعة بابل

Loading...
Loading...
Abstract

The effects of variations in the thermomechanical treatments parameters on the microstructure and mechanical properties of Al-Cu-Mg alloy plates used in aircraft structure subjected to a post heat treatments have been conducted. It was confirmed that a large gain in fracture toughness combined with a good mechanical properties could be achieved by choice of the correct initial condition, amount and temperature of deformation, and the time temperature of the final age hardening sequence. In general, it was found that the material should be age hardened to the peak hardness conditions before deformation at an elevated temperature (warm rolling at 200°C) in order to prompt homogeneous slip. Room temperature deformation resulted in planar slip at the peak hardness conditions non uniform response on subsequent aging and give lower fracture toughness.

تم في هذا ألبحث دراسة ألتأثيرات ألناجمة من تغيير بعض معاملات ألتعامل ألحراري-ألميكانيكي على استجابة سبيكة ألألمنيوم-نحاس-مغنيسيوم ألمستخدمة في هياكل ألطائرات للتقادم ألاصطناعي أللاحق ومتانة ألكسر. وقد ثبت بأن من ألممكن ألحصول على استجابة جيدة ومتانة كسر عالية عن طريق ألاختيار ألصحيح للظروف ألابتدائية كدرجة حرارة وزمن ألتقادم ألأولي،نسبة ودرجة حرارة ألتشويه بالدرفلة وكذلك درجة حرارة وزمن ألتقادم أللاحق. وبصورة عامة فقد وجد بأن ألواح هذه ألسبيكة يجب أن تصلد حتى ألوصول ألىأعلى صلادة ممكنة قبل أن تدرفل بدرجة حرارة (٢٠٠°م) وذلك لتشجيع حصول عملية انزلاق منتظمة لكل ألبنية ألمجهرية. و ثبت أيضا بأن ألعينات ألمدرفلة بدرجة حرارة ألغرفة في ظروف قمة ألصلادة لاتستجيب جيدا لعملية ألتقادم أللاحق وتعطي متانة كسر منخفضة.


Article
Refinement the Microstructure of Al–7Si Alloy by the Addition of Cadmium

Author: Sura Abd Al-Zahrah Muhsion
Journal: Journal of University of Babylon مجلة جامعة بابل ISSN: 19920652 23128135 Year: 2012 Volume: 20 Issue: 1 Pages: 62-66
Publisher: Babylon University جامعة بابل

Loading...
Loading...
Abstract

Cadmium (Cd) modified aluminium–silicon cast alloys are well known for their outstanding mechanical properties as they combine excellent strength with good ductility that is due to a modification of brittle Si in the eutectic with traces of Cd (0.2–1.0 wt%). The results showed that the Cd leads to the refinement of eutectic silicon from ~95 to 10µm. The alloys which used in this work were Al-7Si alloy with additions of 0.2, 0.6 and 1 wt% Cd as well as Al-7%Si with out Cd addition. The effect of keeping time also studied and the results indicate that the addition of 1%Cd with keeping time 3min was the best (about 10 µm).

تكون مصبوبات سبائك الألمنيوم-سليكون، المعدلة بنيتها البلورية بإضافة كميات محسوبة من الكادميوم، ذات خواص ميكانيكية عالية. وهذه الخواص ناتجة عن الجمع بين المتانة العالية والمطيلية الجيدة والناتجة عن تعديل البنية البلورية لطور السليكون الايوتكتيكي من شكل رقائق أو صفائح هشة إلى شكل خيطي منتظم وذلك بفعل إضافة الكادميوم لغاية 1% كمعدل للبنية البلورية. تشير نتائج فحص البنية المجهرية لطور السليكون الايوتكتيكي إلى أن المصبوبة المضاف إليها كادميوم بنسبة 1% قد يصل تحول هذا الطور من شكل ابري أو رقائقي ذو طول حوالي 95 مايكرون إلى خيطي بطول حوالي 10 مايكرون . إن السبائك التي تم دراستها في هذا البحث هي ألمنيوم-7%سليكون بإضافة الكادميوم بنسب(0.2، 0.6 و 1.0%) إضافة إلى السبيكة الأصلية بدون إضافات. كذلك تم دراسة تأثير وقت الحفظ عند درجة حراة إضافة الكادميوم وقد أظهرت النتائج إن المصوبة التي أضيف لها الكادميوم بنسبة 1.0% ووقت حفظ 3 دقائق كانت هي الأفضل (طول السليكون الايوتكتيكي الخيطي10 مايكرون).


Article
EFFECT OF COPPER ADDITION ON THE MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Al-Si ALLOY
تأثير اضافة النحاس على البنية المجهرية والخواص الميكانيكية لسبيكة Al-Si

Author: Yasir Muhi Abdulsahib ياسر محي عبد الصاحب
Journal: Al-Qadisiyah Journal for Engineering Sciences مجلة القادسية للعلوم الهندسية ISSN: 19984456 Year: 2014 Volume: 7 Issue: 4 Pages: 366-381
Publisher: Al-Qadisiyah University جامعة القادسية

Loading...
Loading...
Abstract

Aluminum alloys are very important in many industrial applications because of their lights weight and good mechanical properties. There is a great need to recycle the metals and alloys used in the metallurgical industry and various engineering applications, particularly aluminum alloys due to their low melting point and usefulness. In this work, the effect of copper wires addition with different percent on the microstructure and mechanical properties of Al-Si alloy (piston part as a scrape) were studied. Tensile test, hardness, microstructure SEM and XRD were conducted .The results showed that the addition of copper to the alloy (Al-12wt%Si) have improved its mechanical properties (tensile strength, yield strength and hardness) also changed microstructure of Al-Si alloy as compared with the base alloy

تعتبر سبائك الألومنيوم مهمة جدا في العديد من التطبيقات الصناعية بسبب وزنها الخفيف وخصائصها الميكانيكية الجيدة. هنالك حاجة ماسة لإعادة تدوير المعادن والسبائك المستخدمة في الصناعات المعدنية والتطبيقات الهندسية المختلفة، وخاصة سبائك الألومنيوم بسبب درجة انصهارها المنخفضة واستخداماتها. في هذا البحث تم دراسة تاثير اضافة معدن النحاس على شكل اسلاك بنسب مختلفة على البنية المجهرية والخواص الميكانيكة لسبيكة Al-Si والتي اخذت من مكابس احتراق داخلي لمكائن السيارات (خردة). تم اجراء اختبار الشد والصلادة وكذلك فحص البنية المجهرية باستخدام المجهر الضوئي و فحص حيود الاشعة السينية والفحص باستخدام المجهر الالكتروني الماسح. بينت النتائج ان اضافة النحاس الى سبيكة Al-12wt%Si قد حسنت الخواص الميكانيكية (مقاومة الشد, مقاومة الخضوع والصلادة ) وكذلك تغيرت البنية المجهرية مقارنة بالسبيكة الاساس


Article
FATIGUE BEHAVIORA STUDY OF FERRITIC-MARTENSITIC CRYOGENICALLY TREATED USING 17Mn4 STEEL

Authors: D. A. Alazawi --- B. M. Hussein --- L.E.N. Ekpeni
Journal: DIYALA JOURNAL OF ENGINEERING SCIENCES مجلة ديالى للعلوم الهندسية ISSN: 19998716/26166909 Year: 2015 Volume: 8 Issue: 4 Pages: 731-739
Publisher: Diyala University جامعة ديالى

Loading...
Loading...
Abstract

Based on the importance of impressive mechanical properties good ductility, reduced cost, superior formability and excellent surface finish in terms of Ferritic-martensitic steel, it has been given consideration over other high strength low alloy steels and as such, this research work has been carried out modifying the properties of 17Mn4 Ferritic-martensitic steel.In this work, the 17Mn4 ferritic-martensitic steel specimens were made and cryogenically treated as the first step towards its modification. Fatigue, micro hardness and microstructure inspections were carried out for all treated and non-cryogenic treated 17Mn4 steel specimens. The results showed a significant increase in strength of the 17Mn4 steel compared to the commercial plain carbon steels. From the conducted experiments, the results showed that the fatigue limits for the dual and cryogenic specimens been obtained as (380MPa) and (400MPa) respectively. A considerable enhancement in the fatigue value for the cryogenic steel showed a 6.25%rise as well as the hardness value for the dual and cryogenic treated specimens increasing significantly to (186) and (198) respectively. Further investigation showed a remarkable enhancement in the hardness value to be 25% for the cryo-treated specimen. While the microstructure inspection showed that, the steel containing martensitic with less ferrite grains formed around it, the investigation proved an increment in them artensitic ratio and was seen after the cryogenic treatment was conducted.


Article
Microstructure properties of lead silicate glasses
الخصائص التركيبية لزجاج سلكات الرصاص

Author: Dunia K. M. Al-Nasrawy دنيا كامل مهدي
Journal: Iraqi Journal of Physics المجلة العراقية للفيزياء ISSN: 20704003 Year: 2015 Volume: 13 Issue: 28 Pages: 91-99
Publisher: Baghdad University جامعة بغداد

Loading...
Loading...
Abstract

In the present work, lead silicate glasses have been prepared with different amount of lead oxide content. Structure properties such as X-ray diffraction, AFM, and FTIR analyses have been done. The exceeding of PbO content more than 25wt% revealed a decreasing in density. The X- ray revealed that the strongest peak related to Hexagonal silica dioxide and the other crystal phases formed were related to silica oxide (SiO2) and lead oxide (PbO). Growth and decayed phases in X-ray have been observed with changing lead oxide content. Homogeneous surface was obtained using AFM analyzer with an average diameter around 100 nm. Infrared spectrum is characterized by the presence of large absorption band between 1200 and 900cm-1 and have its maximum at 1080 cm-1 which is typical to stretching vibrations of Si–O–Si bonds, another bands noticed were attributed to Pb–O–Pb, Pb–O–Si, [AlO4]-tetrahedron, and to Si–O–Al bond.

في العمل الحالي، تم تحضير زجاج سيليكات الرصاص وإضافة كميات مختلفة من أوكسيد الرصاص. تم إجراء التحليلات التركيبية مثل حيود الأشعة السينية وميكروسكوب الامتصاص الذري AFMوتحليلات فورير للأشعة الحمراء FTIR. ان زيادة نسبة اوكسيد الرصاص لاكثر من 25 بالمائة أظهرت نقصان في الكثافة. أظهرت نتائج حيود الأشعة السينية ظهور القمة العظمى التي تعود الى سداسي اوكسيد السلكا وبقية الاطور الناشئة تعود الى اوكسيد السلكا واوكسيد الرصاص. تم ملاحظة نمو واضمحلال الأطوار باختلاف محتوى اوكسيد الرصاص بواسطة حيود الأشعة السينية. تم تحليل تجانس السطح بواسطة مايكرو سكوب الامتصاص الذري وبمعدل قطر بحدود 100 نانومتر. تمييز طيف الامتصاص تم بوجود قمة امتصاص كبيرة ما بين 1200 و 900 سم-1 وتمتلك قمة امتصاص عظمى عند 1080 سم-1 والتي تعود نمط اهتزاز الشد لآصرة Si–O–Si, تم ملاحظة أواصر أخرى ترجع الى Pb–O–Pb, Pb–O–Si, ورباعي [AlO4 ] وآصرة Si–O–Al.


Article
Effect of Magnesium Addition on Corrosion Resistance of Aluminum -17%Silicon Alloy
تأثير أضافة المغنيسيوم على مقاومة االتآكل لسبيكة المينيوم – سيليكون 17%

Authors: Muna Khethier Abbass منى خضير عباس --- Khairia Salman Hassan خيرية سلمان حسن --- Kayser Aziz Ameen قيصر عزيز أمين
Journal: Al-Khwarizmi Engineering Journal مجلة الخوارزمي الهندسية ISSN: 18181171 23120789 Year: 2016 Volume: 12 Issue: 4 Pages: 50-58
Publisher: Baghdad University جامعة بغداد

Loading...
Loading...
Abstract

The electrochemical behavior of Al-17%Si alloy is investigated in 3.5wt% NaCl solution. Many alloys with addition of the different wt% magnesium metal of 1wt%, 2%, 3wt% ,4.5wt% ,and 9wt% were prepared by gravity die casting . The microstructures of prepared alloys were examined by optical and SEM microscopes. Corrosion behavior was investigated by using potentiostat instrument under static potentials test and corrosion current was recorded to determine corrosion resistance of all prepared samples. It was found that the addition of Mg metal improves the corrosion resistance of Al-17%Si alloy in 3.5%NaCl solution. The alloy containing 1%Mg shows less corrosion rate than the others while the alloys containing 4.5%Mg, 9%Mg content have the better pitting corrosion resistance than other alloys.

في هذا البحث تم دراسة السلوك الكهروكيمياوي لسبيكة (Al- 17%Si) في محلول (3.5 wt% NaCl)، وذلك باضافة معدن المغنيسيوم للسبائك وبنسب مختلفة (1wt%, 2wt%, 3wt%, 4.5wt%, 9wt%) حيث تم تحضير السبائك بواسطة قوالب الصب بالجاذبية.وقد تم استعمال المجهر الضوئي والمجهر الالكتروني الماسح لفحص التركيب المجهري للسبائك. وتم بحث اسلوب التآكل بواسطة استعمال جهاز المجهاد الساكن (Potentiostat) وتحت اختبار الجهد الساكن وتم تسجيل تيار التأكل وحساب مقاومة التأكل لكل النماذج المحضرة. وقد لوحظ انه عند اضافة معدن المغنيسيوم يزيد من مقاومة التأكل في سبائك (Al-17%Si) في محلول (3.5% NaCl). ولوحظ ايضاً ان السبائك الحاوية على (1% Mg) اظهرت اقل معدل تآكل من السبائك الاخرى بينما كانت السبائك الحاوية على (9% Mg, 4.5% Mg) تمتلك افضل مقاومة للتاكل النقري من باقي السبائك.


Article
Microstructure and Electrical Conductivity of 7075Al alloy/SiC Nano Composites

Authors: Hussain J. Al-Alkawi --- Sameir A. Aziez --- Deana A. Idan
Journal: Engineering and Technology Journal مجلة الهندسة والتكنولوجيا ISSN: 16816900 24120758 Year: 2018 Volume: 36 Issue: 10 Part (A) Engineering Pages: 1034-1038
Publisher: University of Technology الجامعة التكنولوجية

Loading...
Loading...
Abstract

Analysis using scanning electron microscope (SEM) at high magnification showed that the microstructure of the nano composites exhibited uniform distribution of SiC particles and less porosity. The experimental results revealed that adding Nano Reinforcement to 7075Al alloy improve the electrical conductivity for the metal matrix composites with 3, 6, 9 wt. % SiC were adopted in this work. The maximum enhancements were observed at 9wt. %SiC of 5200(Ω. m) -1 compared with the metal base of 35 (Ω. m) -1.


Article
Effect of Lanthanum Addition on the Microstructure ofMg-4Al Alloy
تاثير اضافة معدن اللنثانيوم على خصائص سبيكة المغنسيوم - 4% المنيوم

Author: Ahmed A. Moosa احمد علي موسى
Journal: Al-Khwarizmi Engineering Journal مجلة الخوارزمي الهندسية ISSN: 18181171 23120789 Year: 2011 Volume: 7 Issue: 2 Pages: 75-82
Publisher: Baghdad University جامعة بغداد

Loading...
Loading...
Abstract

This research was to determine the effect of rare earth metal (REM) on the as-cast microstructure of Mg-4Al alloy.
The rare earth metal used here is Lanthanum to produce Mg-4Al-1.5La alloy. The microstructure was characterized by
optical microscopy. The phases of this alloy were identified by X-ray diffraction. The microstructure of Mg-4Al
consists of &#945;-Mg and grain boundaries with precipitated phase particles. With the addition of Lanthanum, three distinct
phases were identified in the X-ray diffraction patterns of the as cast Mg-4Al-1.5La: Mg, Al11La3, Al4La. The Mg17Al12
phase was not detected. The addition of Lanthanium increases the hardness and decrease the wear rate of Mg-4Al.

يهدف هذا البحث الى دراسة تاثير اضافة عناصر الارض النادرة على سبائك (Mg-4Al) والحيلولة دون اكسـدة المغنيسيوم أو احتراقه وأنتاج سبيكة (Mg-4Al-1.5 La).كما تضمن البحث الفحوصات المجهرية وفحص الأشعة السينية لمعرفة الأطوار الناتجة في سبيكة ( (Mg-4Al-1.5 La. أظهرت النتائج أن سبيكة ((Mg-4Al تحتوي على الطور ( α- Mg) مع وجود ترسبات على الحدود البلورية .اما الاطوار في سبيكة ( (Mg-4Al-1.5 La فهي . Mg, Al11La3, Al4La مع عدم ظهور الطور Mg17Al11 . ان اضافة اللنثانيوم يؤدي الى زيادة الصلادة وانخفاض معدل البلى

Listing 11 - 20 of 73 << page
of 8
>>
Sort by
Narrow your search

Resource type

article (73)


Language

English (59)

Arabic (8)

Arabic and English (6)


Year
From To Submit

2019 (5)

2018 (8)

2017 (5)

2016 (7)

2015 (6)

More...