Preparation and Characterization of Chemical Bath Deposition synthesis CdS Nanocrystalline Thin Films
تحضيراغشية CdS النانوية بطريقة الترسيب بالحمام الكيميائي ودراسة خصائصها

Author: H. F. Al-Taay هناء فليح الطائي
Journal: Iraqi Journal of Science المجلة العراقية للعلوم ISSN: 00672904/23121637 Year: 2017 Volume: 58 Issue: 1C Pages: 454-461
Publisher: Baghdad University جامعة بغداد

Loading...
Loading...
Abstract

Cadmium sulfide (CdS) nanocrystalline thin films are prepared onto ITO-glass and Si(111) substrates by chemical bath deposition method. The scanning electron microscope images showed that the CdS thin film onto Si substrate is more homogenous without vacancies. The XRD patterns of the CdS nanocrystalline thin film confirm that they have polycrystalline with cubic phase. Room temperature photoluminescence (PL) spectrum of the CdS nanocrystalline thin films shows emission band located at 502nm for CdS/Si sample while the CdS/ITO-glass thin films shows a broad emission band peaked at 505nm. The Raman spectra of CdS nanocrystalline thin films prepared onto Si and ITO-glass substrates contain two main peaks which are corresponding to the first and second-order longitudinal optical (LO) phonon modes.

حضرت اغشية المركب CdS نانوية التركيب علىى قواعد ITO-glass و(111) Si بطريقة الترسيب بالحمام الكيمائي. اظهرت صور المجهر الالكتروني الماسح ان اغشية المركب المرسبة على السليكون كانت اكثر تجانسا وقليلة الفراغات. انماط حيود الاشعة السينية بينت ان الاغشية المحضرة كانت متعددة التبلور وبتركيب مكعب. طيف الانبعاثية الضوئيةPL)) لاغشية CdS/Si تمركز عند الطول الموجي 502 نانومتر بينما كان طيف الانبعاثية عريضا لاغشية المركب CdS/ITO مع التمركز عند الطول الموجي 505 نانومتر. انماط رامان لكلا النموذجين المحضرين على قواعد Si وقواعد ITO اظهرت قمتان رئيستان تعودان للنمطين الاول والثاني من الدرجة الطولية لنمط ضوئية-صوتية.


Article
Fabrication and characterization of porous CdS/dye sensitized solar cells
تحضير خصائص خلايا الصبغات الشمسية المصنوعة من المركب CdS النانوي التركيب ودراستها

Loading...
Loading...
Abstract

Dye sensitized solar cells (DSSCs) were fabricated from porous cadmium sulfide (CdS) nanocrystalline thin films. The porous CdS nanostructured thin films were deposited onto FTO/glass substrates by the chemical bath deposition (CBD) method. The surface morphology, crystalline structure, and optical properties of the prepared nanocrystalline thin films were investigated. Rhodamine B, Malachite green, Eosine methylene blue, and Cresyl violet dyes were used to fabricate the DSSC devices. Comparing by the absorption spectrum of the prepared porous CdS nanocrystalline films, all dyes showed an absorption peak in the transparent range of CdS thin films indicating that they are suitable for the preparation of DSSCs with CdS. Current-voltage (I-V) characteristics showed that the fabricated solar cell using malachite green dye had the highest conversion efficiency of 0.83% while using Rhodamine B dye produces a solar cell with lowest efficiency of 0.38%. However, heat treatment to the fabricated solar cells caused significant enhancement in the output of all devices.

ان تحضير خصائص المواد نانوية التركيب ودراستها يُعد غاية بالاهمية وذلك للخصائص الفريدة التي امتازت بها دون المواد الاخرى. المميزات الفريدة وخاصة الزيادة الكبيرة جداً في نسبة المساحة السطحية الى الحجم جعلت من هذه المواد تدخل في تصنيع كثير من النبائط الالكترونية وخصوصاً الخلايا الشمسية. في دراستنا هذه، حُضرت اغشية المركب CdS النانوية التركيب على قواعد موصلة وشفافة FTO باستخدام تقنية الترسيب الكيميائي Chemical Bath) Deposition (CBD) . بينت فحوصات المجهر الاكتروني FE-SEM ان الاغشية المحضرة بتقنية CBD كانت اغشية اسفنجية التركيب Porous . حُضرت خلايا شمسية باستخدام اربع صبغات هي Rhodamine B، Malachite green، Eosin-methylene blue، و Cresyl violet perchlorate. اظهرت الخلايا الشمسية المحضرة باستعمال عينة CdS الاسفنجي كفاءة تحويل اعلى من خلايا تركيب الجدران النانوية التركيب, اذ كانت اعلى كفاءة تحويل حُصل عليها 0.82% لصبغة Malachite green. المعاملة الحرارية للخلايا المحضرة وادت الى تحسن كفاءة التحويل بشكل كبير لكلا النوعين اذ بلغت اقصى قيمة لخلية Cresyl violet باستعمال غشاء CdS الاسفنجي .1.25%.

Listing 1 - 2 of 2
Sort by
Narrow your search

Resource type

article (2)


Language

English (2)


Year
From To Submit

2017 (1)

2016 (1)