Study the Impact Behavior of the Prosthetic Lower Limb Lamination Materials Due to Low Velocity Impactor
دراسه سلوك الصدم الواطئ السرعه للمواد المركبه المستخدمة في صناعه وقب الطرف الصناعي لبتر تحت الركبه

Author: Jumaa Salman Chiad جمعه سلمان جياد
Journal: Journal of Engineering مجلة الهندسة ISSN: 17264073 25203339 Year: 2014 Volume: 20 Issue: 4 Pages: 82-98
Publisher: Baghdad University جامعة بغداد

Loading...
Loading...
Abstract

This work involves three parts , first part is manufacturing different types of laminated below knee prosthetic socket materials with different classical laminated materials used in Baghdad center for prosthetic and orthotic (4perlon layers+2carbon fiber layer+4 perlon layers) , two suggested laminated materials(3perlon layers+2carbon fiber layer+3 perlon layers) and (3perlon layers+1carbon fiber layer+3 perlon layers) ) in order to choose perfect laminated socket . The second part tests (Impact test) the laminated materials specimens used in socket manufacturing in order to get the impact properties for each socket materials groups using an experimental rig designed especially for this purpose. The interface pressure between the residual leg and prosthetic socket is also measured to cover all the surface area of the B-K prosthetic socket by using piezoelectric sensor in order to estimate the resulting stress according to loading conditions . A male with age, length, mass, and stump length of 42 years, 164 cm, 67 Kg and 13 cm respectively with a right transtibial amputation is chosen to achieve the above mentioned test procedures. The last part suggests a theoretical and analytical models for each group of specimen to find out the absorbed energy behavior and subjected maximum stress for each laminated B-K prosthetic socket materials .

يتضمن هذا العمل ثلاثة اجزاء رئيسية الاول شمل تصنيع وقب طرف صناعي وفق طريقة الخلط وعدد الطبقات المستخدمة كلاسيكيا في مركز بغداد للاطراف الصناعية وهي (4طبقة برلون+2طبقة كاربون فايبر +4 طبقة برلون) وايضا تم اقتراح نموذجين اخريين هما (3طبقة برلون+2طبقة كاربون فايبر +3 طبقة برلون) و(3طبقة برلون+1طبقة كاربون فايبر +3 طبقة برلون) .اما الجزء الثاني فكان تصنيع وفحص العينات لمختلف الفحوصات الميكانيكية كفحص الشد بالاضافة الى فحص الصدم من خلال استخدام منظومة فحص صممت وصنعت لغرض اجراء فحص الصدم الواطئ السرعة للمواد المركبة المستخدمة في تصنيع وقب طرف صناعي لبتر تحت الركبة.كما تم قياس ضغط التلامس بين وقب الطرف الصناعي ومتبقي الطرف لحالة بحثية تعرضت لبتر تحت الركبة بعمر 42سنة وطول 164 سم ووزن 67 كيلوغرام وطول بتر 13 سم من خلال استخدام منظومة قياس ضغط التلامس صممت وصنعت لهذا الغرض بهدف حساب الاجهادات التي يتعرض لها الطرف الصناعي اثناء تعرضة لظروف العمل المختلفة.الجزء الثالث والاخير تضمن اقتراح حل نظري ونموذج عددي للحالة البحثية لكل مجموعة من العينات لكل مادة مقترحة لتصنيع وقب الطرف الصناعي لايجاد سلوك الطاقة المخزونة وايجاد الاجهاد الاعظم الذي يتعرض له وقب الطرف الصناعي اثناء الخدمة وظروف التحميل المختلفة .


Article
Experimental Study for Materials Prosthetic above Knee Socket under Tensile or Fatigue Stress with Varying Temperatures Effect
دراسة عملية لمواد وقب طرف سفلي صناعي أعلى الركبة تحت تأثير أجهاد الشد أو الكلال عند مختلف درجات الحرارة

Authors: Hatem Rahim Wasmi حاتم رحيم وسمي --- Jumaa Salman Chiad جمعه سلمان جياد --- Adawiya Ali Hamzah عدويه علي حمزه
Journal: Journal of Engineering مجلة الهندسة ISSN: 17264073 25203339 Year: 2014 Volume: 20 Issue: 3 Pages: 87-95
Publisher: Baghdad University جامعة بغداد

Loading...
Loading...
Abstract

The residual limb within the prosthesis, is often subjected to tensile or fatigue stress with varying temperatures. The fatigue stress and temperatures difference which faced by amputee during his daily activities will produces an environmental media for growth of fungi and bacteria in addition to the damage that occurs in the prosthesis which minimizingthe life of the prosthetic limb and causing disconfirm feeling for the amputee. In this paper, a mechanical and thermal properties of composite materials prosthetic socket made of different lamination for perlon/fiber glass/perlon, are calculated by using tesile test device under varying temperatures ( from 20oC to 60oC), also in this paper a device for measuring rotational bending fatigue stress under varying temperatures was designed, manufactured, and calibrated ( this device is not available in Iraq), to achieve S – N curves for different lamination of perlon/fiber glass/perlon composite materials of prosthetic above knee socket. In this paper, the mechanical and thermal properties set ( E, σy, σult, K, and α ) results of the above composite materials are decreased when the temperatures are increased. The S–N curves results of rotational bending fatigue for these lamination of composite materials are decreased when the temperatures are increased,also the endurance limit stresses (σe) are decreased with the increasing of number of perlon, and increasing temperatures, generaly after about 107 cycles.

يتعرض متيقي العضو المبتور الى اجهاد شد أو كلال متكرر مع اختلاف في درجات الحرارة بشكل دائم. ان تعرض الطرف المبتور الى اجهاد كلال متكرر ودرجات الحرارة المختلفة يسبب في كثير من الأحيان بيئة لنمو الفطريات والبكتريا ناهيك عن الضرر الذي يتعرض له متبقي الطرف المبتور بالأضافة الى الضرر الذي يحدث في الطرف الصناعي مما يسبب عدم راحة ذوي الأحتياجات الخاصة بالأضافة الى قصرعمرالطرف الصناعي. في هذا البحث تم أستخراج الخواص الميكانيكية والحرارية للمواد المركبة الداخلة في تصنيع وقب طرف سفلي صناعي أعلى الركبة مصنع من البرلون/ألياف الزجاج/البرلون ذو طبقات مختلفة وذلك بأستخدام جهاز أختبار شد معرض الى درجات حرارة مختلفة ( من 20 الى 60 درجة مئوية). كذلك تم في هذا البحث تصميم وتصنيع ومعايرة جهاز أختبار كلال أنحناء دوراني حراري (الجهاز غير متوفر في العراق) وذلك لغرض استخراج منحنيات الأجهاد – عدد الدورات للوصول الى الفشل لطبقات مختلفة من المواد المركبة برلون / ألياف الزجاج / برلون المصنوع منها وقب الطرف الصناعي. أن نتائج الخواص الميكانيكية والحرارية التي أستخرجت في هذا البحث مثل (معامل المرونة وأجهاد الخضوع وأجهاد الشد الأعظم والمتانة ومعامل التمدد الحراري) للمواد المركبة التي ذكرت أعلاه تقل مع أرتفاع درجات الحرارة. كذلك وجد بأن نتائج منحنيات الأجهاد – عددالدورات للوصول الى الفشل من خلال أختبار أجهاد كلال الأنحناء الدوراني لصفائح المواد المركبة المذكورة تقل مع أرتفاع درجات الحرارة. كذلك وجد أن اجهادات حد التحميل تقل مع زيادة عدد طبقات البرلون وأرتفاع درجات الحرارة بعد حوالي عشرة ملايين دورة.


Article
Reduction the Effects of the Vibration Parameter on the Replacement Knee Joint during Daily Gait Cycle
الحد من آثار معلمة الاهتزاز على مفصل الركبة البديلة أثناء دورة المشي اليومية

Authors: Jumaa Salman Chiad جمعه سلمان جياد --- Noor Dhia Yaseen نور ضياء ياسين --- Firas Mohammed Abdul Ghani فراس محمد عبدالغني
Journal: AL-NAHRAIN JOURNAL FOR ENGINEERING SCIENCES مجلة النهرين للعلوم الهندسية ISSN: 25219154 / eISSN 25219162 Year: 2018 Volume: 21 Issue: 4 Pages: 486-493
Publisher: Al-Nahrain University جامعة النهرين

Loading...
Loading...
Abstract

There are many patients who face a lot of things that hurt the knee joint. Knee replacement is the best solution to these problems. This research was based on reducing the vibrations of daily activities as measured by the frequency of foot and knee for the patient for three cases when the bare foot, sports shoes with ground air and sports shoes with ground air with silicon damping. Patient information for this work was of age, weight, height and leg length 48 years, 90 kg, 160 cm, 84 cm, respectively. The results was shown that the decline in acceleration results was in the case of sport shoes with ground air with silicon damping with 22.57%, while the decline in vibration results was in the case of sports shoes with ground air with -54.9%.

هناك العديد من المرضى الذين يواجهون الكثير من الأشياء التي تؤذي مفصل الركبة. استبدال الركبة هو الحل الأفضل لهذه المشاكل. استند هذا البحث إلى تقليل الاهتزازات في الأنشطة اليومية حسب قياس وتيرة القدم والركبة للمريض لحالتين عند القدم العارية وفي حالة الأحذية الرياضية مع الهواء الأرضي. معلومات المريض لهذا العمل هي من العمر والوزن والطول وطول الساق 48 سنة ، 90 كجم ، 160 سم ، 84 سم ، على التوالي. وجد أن الانخفاض في نتائج التسارع كان في حالة الأحذية الرياضية مع الهواء الأرضي مع التخميد السليكوني بنسبة 22.57٪ ، في حين كان الانخفاض في نتائج الاهتزاز في حالة الأحذية الرياضية مع الهواء الرياضي مع -54,9%.