Enhancing Reological Properties of liquid asphalt

Authors: . Dr. Firyal Mohammed Ali فريال محمد علي --- Zena A.H --- Omar M. Khalel
Journal: Journal of Petroleum Research & Studies مجلة البحوث والدراسات النفطية ISSN: 22205381 Year: 2017 Issue: 17 Pages: E39-E50
Publisher: Ministry of Oil وزارة النفط

Loading...
Loading...
Abstract

The purpose of this study is to improve the specifications of cut back asphalt (S125) in order to use in the treatment of holes, potholes and cracks of roads. Different methods were carried out to enhance physical and mechanical properties and to get better construction behavior. These treatments are:-First: The vacuum distillation of S125 cut back asphalt was employed to remove oil, vacuum gas oil and vacuum residue as a rapid curing. FTIR spectra of the four fractions of S125 were recorded. It was observed a low penetration and high softening point for the vacuum residue.Second: extraction method using ethanol as a solvent was employed to extract light component that could be in the S125 cut back asphalt. The results indicated that the softening point was highly increased and the penetration as well as ductility was decreased to minimized level.Third: Some Polymers were used as cross linking agent such as melamine and phenol formaldehyde resins. Fourth: The unsaturated monomers were polymerized free radically to increase the solidification of S125. Fifth: The hydrated white cement was used as additive to the S125 cutback asphalt at different ratios to improve the properties. This method was observed as a suitable and economic method, and easy employed compared to others and the best rheological behaviors were given in this method. Also the vacuum distillation method gave high improvements in rheological properties for asphalt residue.


Article
The Use Of Liquid Asphalt To Improve Gypseous Soils
استخدام الاسفلت السائل لتحسين التربة الجبسية

Journal: AL Rafdain Engineering Journal مجلة هندسة الرافدين ISSN: 18130526 Year: 2008 Volume: 16 Issue: 4 Pages: 38-48
Publisher: Mosul University جامعة الموصل

Loading...
Loading...
Abstract

This work aimed to study the effectiveness of liquid asphalt in the enhancement of gypseous soils properties. This enhancement is by reducing the effect of water on gypsum particles and increasing strength parameters.The work included two types of treatments firstly is by mixing technique and the second type is by grouting technique.The testing program included the determination of unconfined compressive strength, shear strength and collapsibility parameters of untreated and treated gypseous soil with different percent of liquid asphalt.The test results showed that the maximum unconfined compressive strength and the shear strength of soil increased to an optimum value and then decreased with increasing liquid asphalt.The study concluded that the mixing technique was better than the injection technique because the mixing technique will cover the particles with a film of asphalt while the injection fills the voids of soil with asphalt. Moreover the results show that the oblique injection gives more strength to the soil than normal injection.Keywords: Gypseous soil, Liquid asphalt, Soil improvement, Grouting, Injection

الخلاصةان الهدف الرئيسي من هذه العمل هو دراسة تأثير الإسفلت السائل (cut-back RC-70) في تحسين خواص التربة الجبسية. حيث هذا التحسين يكمن في تقليل تأثير الماء على حبيبات الجبس المتواجدة في التربة والتي تعمل كمادة رابطة في التربة وكذلك في زيادة مقاومة التربة الجبسية.في هذا العمل تم اجراء نوعين من المعالجة النوع الاول المعالجة بواسطة الخلط اليدوي والنوع الثاني المعالجة بواسطة الحقن.تضمنت الدراسة اجراء فحص مقاومة الانضغاط غير المحصور وكذلك أجراء فحص القص المباشر لايجاد تماسك التربة وزاوية الاحتكاك الداخلي لها واخيرا" فحص الانهيارية. حيث أجريت جميع هذه الفحوصات للترب غير المعالجة والمعالجة بنسب مختلفة من الإسفلت في حالة الجفاف وحالة الغمر بالماء. اوضحت النتائج ان مقاومة الانضغاط غير المحصور للتربة تزداد قيمتها (حوالي 33%) عند النسبة المثلى للمعالجة وهي (6%) ومن ثم تتناقص بزيادة محتوى الاسفلت. كذلك فان تماسك التربة يزداد بزيادة محتوى الاسفلت الى القيمة العظمى و من ثم تتناقص بزيادة محتوى الاسفلت. عند غمر التربة بالماء لوحظ تناقص قيم الانضغاط غير المحصور و كذلك تماسك التربة. كما بينت النتائج ان الحقن المائل تفضل من الحقن العمودي.استنتج من هذه الدراسة انه طريقة الخلط اليدوي للسفلت مع التربة افضل من طريقة الحقن بسبب كونها طريقة مثالية حيث يتم تغطية حبيبات التربة بطبقة قليلة من الاسفلت في حين ان طريقة الحقن يتم فيها ملء فجواة التربة بالاسفلت


Article
Influence of Liquid Asphalt on Resilient Modules and Permanent Deformation of Recycled Asphalt Concrete
تأثير الاسفلت السائل على معامل المرونة والتشوه الدائمي للخرسانة الاسفلتية المعاد تدويرها

Authors: Mohammed Chaloob Saleem AL-Shujairy محمد جلوب سليم الشجيري --- Saad Isaa Sarsam سعد عيسى سرسم
Journal: Journal of Engineering مجلة الهندسة ISSN: 17264073 25203339 Year: 2019 Volume: 25 Issue: 9 Pages: 76-91
Publisher: Baghdad University جامعة بغداد

Loading...
Loading...
Abstract

Tests were performed on Marshall samples and were implemented for permanent deformation and resilient modulus (Mr) under indirect tensile repeated loading (ITRL), with constant stress level. Two types of liquid asphalt (cutback and emulsion) were tried as recycling agents, aged materials that were reclaimed from field (100% RAP), samples were prepared from the aged mixture, and two types of liquid asphalt (cutback and emulsion) with a weight content of 0.5% were utilized to prepare a recycled mixture. A group of twelve samples was prepared for each mixture; six samples were tested directly for ITRL test (three samples at 25˚C and three samples at 40˚C), an average value for ITRL for every three samples was calculated (ITRL for unconditioned samples). The other six samples were placed in volumetric flask 4000-ml heavy- wall glass filled with water at 25˚C under a vacuum pressure of (3.74 kPa) for 5 to 10 minutes. Then the samples were put in deep freeze for 16 hours at -18˚C. The samples were frozen then were transported to a water bath at 60ºC for 24 hours. Then they were soaked in a water bath for 1 hour at 25ºC and tested for the ITRL test (three samples at 25˚C and three samples at 40˚C), the average value of ITRL for every three samples was calculated (ITRL for conditioned samples). It was concluded that the reduction in (Mr) at the Conditioned test as compared to the Unconditioned test was (29.5%, 22.27% and 9.09%) at 25˚C, while at 40˚C, the reduction was (21.28%, 15.53%, and 17.89%) for aged and recycled mixtures with (cutback), and (emulsion) respectively. The change in permanent deformation at the Conditioned test as compared to Unconditioned one was (76.19%, 75.61% and 53.22%) at 25˚C, while at 40˚C it was (56.48%, 35.19%, and 78.33%) for aged and recycled mixtures with (cutback), and (emulsion) respectively.

اجريت الاختبارات على عينات مارشال، وتم تنفيذها لإيجاد التشوه الدائم ومعامل المرونة تحت الاحمال المتكررة للشد غير المباشر مع مستوى اجهاد ثابت. سيتم اختبار نوعين من الاسفلت السائل (القطران والمستحلب السائل) كعوامل إعادة تدوير للمواد القديمة التي تم الحصول عليها من الموقع بنسبة(100)% .وسيتم تحضير النماذج من الخلطة القديمة ونوعين من معاملات التدوير(القطران والمستحلب السائل)وبنسبة (0.5)% من وزن الخلطة لاستخدامها كمعاملات لإعادة التدوير. وتم اعداد اثني عشر عينة لكل خليط، واختبرت ست عينات مباشرة لاختبار الاحمال المتكررة للشد غير المباشر(ثلاث عينات بدرجة 25 مئوية وثلاث عينات بدرجة 40 مئوية)و حساب معدل القيمة لكل ثلاث عينات (الشد غير المباشر للأحمال المتكررة غير معرض لضرر الرطوبة).العينات الست الاخرة وضعت في قارورة حجمية 4000 مل ذات جدران زجاجية سميكة مملؤة بالماء بدرجة 25 مئوية تحت ضغط الفراغ من (3.74 كيلو باسكال) لفترة(5الى 10) دقيقة. ثم وضعت العينات في تجميد عميق لمدة 16 ساعة في درجة (-18) مئوية ونقلت العينات المجمدة بعد ذلك الى حمام مائي عند 60 درجة مئوية لمدة 24 ساعة. ثم غمرت في الماء لساعة واحدة بدرجة 25 مئوية واختبرت العينات لاختبار الشد غير المباشر تحت الاحمال المتكررة (ثلاث عينات بدرجة 25 مئوية وثلاث عينات بدرجة 40 مئوية) و حساب معدل القيمة لكل ثلاث عينات (الشد غير المباشر للأحمال المتكررة معرض لضرر الرطوبة) واستنتج ان الانخفاض في معامل المرونة للفحص المعرض لضرر الرطوبة بالمقارنة مع الفحص الغير معرض لضرر الرطوبة كان(29.5% ،22.27 % و 9.09%) في درجة 25 مئوية. بينما في درجة 40 مئوية الانخفاض كان( 21.28% ، 15.53% ، و 17.89% ) للخلطة القديمة والخلطات المعاد تدويرها مع(القطران والمستحلب السائل )على التوالي. وكان التغير في التشوه الدائم للاختبار المعرض لضرر الرطوبة بالمقارنة مع الاختبار الغير معرض لضرر الرطوبة (76.19% ، 75.61% و 53.22% ) في درجة 25 مئوية ، بينما في درجة 40 مئوية كان (56.48% ، 35،19% و 78.33% ) للخلة القديمة والخلطات المعاد تدويرها مع (القطران والمستحلب السائل ) على التوالي.

Listing 1 - 3 of 3
Sort by
Narrow your search

Resource type

article (3)


Language

English (3)


Year
From To Submit

2019 (1)

2017 (1)

2008 (1)