Synthesis of TiO2 and Cu2O nanoparticles and TiO2/Cu2O nanocomposite and study the ability to remove pollutants from aqueous solution
تخليق جسيمات Cu2O,TiO2 النانوية ومتراكباتها Cu2O/TiO2 ودراسة قابليتهم لازالة الملوثات من محاليلها المائية

Author: Shaimaa hamed jaber
Journal: journal of kerbala university مجلة جامعة كربلاء ISSN: 18130410 Year: 2017 Issue: المؤتمر العلمي الخامس لكلية العلوم Pages: 137-146
Publisher: Kerbala University جامعة كربلاء

Loading...
Loading...
Abstract

TiO2,Cu2O nanoparticles and TiO2/Cu2O nanocomposite have been synthesized by electrochemical deposition method. The synthesized nanoparticles and nanocomposite characterized by X-ray diffraction (XRD), Transmission Electron Microscopy (TEM) and Scanning Electron Microscopy (SEM). Results showed that TiO2 nanoparticles have average size of (8-14)nm, Cu2O nanoparticles have average size of (11-15)nm and TiO2/Cu2O nanocomposite have average size of (13-20)nm. The synthesized nanoparticles were applied to remove 1-nitroso-2-naphthol from aqueous solution. UV-vis spectra results indicate that the percentage of degradation with the sequence TiO2/Cu2O= 89%< TiO2= 68% < Cu2O= 42% .

تم تخليق اوكسيد التيتانيوم النانوي(TiO2)،اوكسيد النحاس النانوي (Cu2O) والمتراكب النانوي من جسيمات Cu2O/TiO2 بطريقة الترسيب الكهروكيميائي وبفرق جهد مقداره 3 فولت. شخصت هذه الجسيمات النانوية باستخدام تقنية حيود الاشعة السينية، المجهر الالكتروني النافذ والمجهر الالكتروني الماسح . حيث كان متوسط الحجم للجسيمات النانوية لاوكسيد التيتانيوم nm(14-8)، ولاوكسيد النحاسnm( 15-11) وللمتراكب nm( 20-13). أظهرت نتائج طيف الاشعة الفوق البنفسجية والمرئية فعالية عالية في التحفيز الضوئي للجسيمات النانوية Cu2O,TiO2 وجسيمات النانو Cu2O/TiO2 المتراكب في معالجة الماء المتلوث بمادة 1-nitroso-2-naphthol حيث كانت النسب المئوية للازالة بالتسلسل :TiO2/Cu2O= 89%< TiO2= 68% < Cu2O= 42% .


Article
Cu2O nanoparticles preparation by Pulse Laser Ablation in Liquid Phase method (PLALP)
تحضير جسيمات نانوية لأوكسيد النحاس الأحادي بطريقة الاستئصال بالليزر النبضي في وسط مائي (PLALP)

Loading...
Loading...
Abstract

The Nanoparticles has pulled in expanding consideration with the developing enthusiasm for nanotechnology which hold potential as essential segments for development applications. In the present work, a cuprous oxide nanoparticles are manufactured as a suspension in distilled water by bombarding a bulk copper target with laser source (532 nm wavelength, 10 ns pulse duration and 10 Hz repletion rate) via method. UV- visible absorption spectra, an AFM analysis has been done. Copper oxide nanoparticles (Cu2O-NPs) with dark color are successfully synthesized. The Cu¬2O- NPs have very high purity because the preparation was managed in aqueous media to eliminate ambient contaminations. Absorption spectrum shows peaks at 450 nm- 700 nm due to the generation of Cu Oxides-NPs.

حظيت جسيمات بحجم النانو باهتمام واسع مع التطور في نشاطات تقانة النانو والتي ثبتت نفسها في قطاعات اساسية للتطبيقات التطويرية. في هذا العمل حضرت جسيمات نانوية لأوكسيد النحاس الاحادي كمعلق في وسط مائي مقطر بقصف كتلة نحاس كهدف لمصدر اشعة ليزر (532 نانومتر طول موجي، 10 نانو ثانية زمن النبضة، بمعدل تكرار 10 هرتز). أجريت فحوص طيف الامتصاص للجزء المرئي وفوق البنفسجية و تحليل مجهر القوة الذرية AFM. حضرت بنجاح جسيمات نانوية لاوكسيد النحاس الأحادي وكانت بلون غامق. وكانت الجسيمات عالية النقاوة لانها حضرت في وسط مائي من اجل منع التلوث المحيط بها. أظهر طيف الامتصاص القمم بين 450 نانومتر و700 نانومتر وهذا تبعا لتكون جسيمات نانوية الحجم لاوكسيد النحاس الاحادي.