Analysis of mechanical properties of randomly oriented phenol composites
تحليل الصفات الميكانيكية لمركبات الفينول عشوائية الاتجاه

Author: Faiza M. Salim
Journal: Diyala Journal For Pure Science مجلة ديالى للعلوم الصرفة ISSN: 83732222 25189255 Year: 2011 Volume: 7 Issue: 3 Pages: 71-85
Publisher: Diyala University جامعة ديالى

Loading...
Loading...
Abstract

Tensile strength, compression strength, bending strength, and fracture toughness of phenolformaldehyde type novolac resin (PFN) reinforced with randomly-oriented different fibers aswell as powders in terms of mechanical properties, which are subject to change in differentadditives volume fraction have been studied. Tensile strength, σT , results show that σTincreases with the increasing volume fraction of additives. Failures display two mechanismsaccording to the kind of additives. Where, it can be observed, pullout mechanism with respectto fibers composites, and rupture mechanism with respect to powder fillers composites.Compression strength, σc , results show that σc increases with the increasing volume fractionof additives. Bending strength, σf, results show, that σf increases progressively by successionof volume fraction of fibers. Fracture toughness Gc , results show that Gc increased withincreasing of volume fraction of additives. Failure takes place through two mechanisms,according to additives kind. Where, the failure takes place by pullout mechanism with respectto fibers composites, and by pining mechanism with respect to powder fillers composites.

تم دراسة قوى الشد والانضغاط والانحناء والصلابة لمادة الفينول – فورمالديهايد نوع نوفولاك راتنجي معزز بألياف عشوائية الاتجاه ومساحيق مختلفة كدالة لنسب اضافة هذه المواد. بينت النتائج ان قوة الشد تزداد بزيادة نسبة المواد المضافة وقد بين الفشل وجود اليتين اعتمادا على نوع المواد المضافة حيث تم ملاحظة الية السحب في حالة المركبات ذات الالياف والية التمزق في حالة المركبات ذات المساحيق. كما بينت النتائج ان قوة الانضغاط والانحناء والصلابة تزداد ايضا بزيادة نسبة المواد المضافة.


Article
Mechanical and physical properties of carbon nanotubes with Kevlar fiber reinforced with polyester resin
الخواص الميكانيكية و الفيزيائية لانابيب الكاربون النانوية مع الياف الكفلر المقواة مع راتنج البولي استر

Loading...
Loading...
Abstract

In this research study Hardness (shore D), Water absorption, Flexural, Impact Test, and Fracture Toughness of polymer nano composites.The polymer nano composites based on unsaturated polyester resin reinforced with Kevlar fibers (K.F). The samples are attended by hand lay – up method according to (Rule mixture) for various volume fractions of unsaturated polyester resin, fiber and carbon nanotube. The polyester resin was matrix strengthened with 3% volume fraction from Kevlar fiber and (0.5%, 1%, 1.5%, 2%( volume fractions of carbon nanotube. The water absorption, hardness (shore D), flexural test, impact testand toughness fracture properties were studied. Results showed that the water absorption increase with volume fraction increase of fiber with Carbon Nanotube, the sample (polyester+3%K.F+0.5% CNTs) has lower water absorption than other samples. The hardness (shore D), flexural test, impact testand toughness fracture for the sample (polyester+3%C.F+0.5% CNTs) has higher value for Nano- composites. Nano composites, Carbon nanotube, Kevlar fiber, Hardness (shore D), Water absorption, Flexural Strength, Impact Test, Toughness Fracture.

تم في هذا البحث دراسة الصلادة (شورD), امتصاصية الماء, مقاومة الكسر, اختبار الصدمة و متانة الكسر لمتراكبات نانوية ذات اساس راتنج البولي استر غير المشبع مقواة بألياف الكفلر. العينات جهزت بطريقة الصب اليدوي وفقالقاعدة الخلط لكسور حجمية مختلفة من راتنج البولي استر غير المشبع والالياف وانابيب الكاربون النانوية. راتنج البولي استر كان ارضية مقواة مع 3%كسر حجمي من الياف الكفلر و (0.5 ,1 ,1.5 , 2 ) % كسر حجمي لانابيب الكاربون النانوية. تم دراسة خواص امتصاصية الماء, صلادة (شور(D, اختبار الصدمة ومقاومة الكسر. اظهرت النتائج بان امتصاصيه الماء تزداد مع زيادة الكسر الحجمي للالياف مع انابيب الكاربون النانوية, العينه (بولي استر + 3% الياف كفلر + 0.5 % انابيب اكاربون النانوية) تمتلك اقل امتصاصية ماء من العينات الاخرى. الصلادة (شورD), فحص الكسر, فحص الصدمة ومتانة الكسر للعينه (بولي استر +3% الياف كفلر + 0.5 %انابيب الكاربون انانوية) تمتلك اعلى قيمه للمتراكبات النانوية.

Listing 1 - 2 of 2
Sort by
Narrow your search

Resource type

article (2)


Language

English (2)


Year
From To Submit

2016 (1)

2011 (1)