research centers


Search results: Found 8

Listing 1 - 8 of 8
Sort by

Article
Structure and Some Optical Properties of ZnS Thin Films Prepared by Thermal Evaporation Method.

Author: J. J. Hassan
Journal: Journal of Basrah Researches (Sciences) مجلة ابحاث البصرة ( العلميات) ISSN: 18172695 Year: 2006 Volume: 32 Issue: 3A Pages: 61-69
Publisher: Basrah University جامعة البصرة

Loading...
Loading...
Abstract

Zinc sulfide thin films were prepared by thermal evaporation technique, on glass substrate(corning 7059) at different substrate temperatures. Films structure and grain size were determined by X-ray diffraction (XRD) device. Films have cubic polycrystalline structure with lattice constant . The optical constants (refractive index and absorption coefficient) of the films were derived from optical transmission spectra in the wavelength range 300-700 nm. Data are analyzed by Swanepoel method. Increasing of substrate temperature, the refractive index of films was increased and all films have nearly same refractive index at wavelength about 630 nm. Optical band of prepared films are in the range 3.4-3.62 eV and was increased with increasing substrate temperature. The aim of this study is to obtain matched properties from ZnS thin films to be used in solar cell applications.

حضرت أغشية كبريتيد الخارصـــين بوســـــاطة تقنـية التبخـــير الحراري بالــفراغ على قواعــد مــــن الزجـــاج(corning 7059) وعند درجات حرارة قاعدة مختلفة.التركيب البلوري والحجم الحبيبي حسب بأستخدام تقنية الاشعة السينية(XRD) .الاغشية المحضرة تملك تركيباً مكعباً متعدد التبلور وبثابت شبيكي قدره الثوابت الضوئية(معامل الانعكاس ومعامل الامتصاص) لهذه الاغشية استحصلت من طيف النفاذية في المدى 300-700 nm .بيانات النفاذية حللت بأستخدام طريقة Swanepoel.حيث ان معامل الانعكاس يزداد مع زيادة درجة حرارة قاعدة اترسيب وجميع الاغشية المحضرة تملك تقريباً نفس معامل الانعكاس بالقرب من الطول الموجي 630 nm .فجوة الطاقة للاغشية المحضرة تتراوح بين 3.4-3.62 eV حيث انها تزداد مع زيادة حرارة قاعدة الترسيب .الهدف من الدراسة هو الحصول على اغشية ZnS ذات خصائص ملائمة لاستخدامها في تطبيقات الخلايا الشمسية.


Article
Structure and Optical Properties of ZnCdO Thin Films Prepared by Spray Pyrolysis

Author: Jabbar H. Khlaief
Journal: Al-Nahrain Journal of Science مجلة النهرين للعلوم ISSN: (print)26635453,(online)26635461 Year: 2016 Volume: 19 Issue: 3 Pages: 77-86
Publisher: Al-Nahrain University جامعة النهرين

Loading...
Loading...
Abstract

ZnCdO films were compounded by spray pyrolysis on glass substrates at temperature of 250Co, using solution of zinc acetate and cadmium acetate salts with various additions concentrations of Zn (25, 50, 75)%. Structure and optical properties have been analyzed using XRD and UV-Vis spectroscopy. XRD analysis premiered that thin films were of polycrystalline nature with face centered cubic structure. The crystallinity increases when the Zn additions increases. Film additions with 75% Zn has minimum value of dislocation density and strain which confirm the improved crystallinity of the film. The optical results featured the transparency of the ZnCdO films is greater than 80% in the visible region, and we found when the concentration of Zn additions increase the optical band gap increasing from (2.49 to 2.9eV).

اغشية اوكسيد الكادميوم-الزنك تم تحضيرها بطريقة الرش الكيميائي الحراري على قواعد من الزجاج وبدرجة حرارة 250 درجة مئوية، باستخدام محاليل لاملاح الكادميوم والزنك وبنسب اضافة مختلفة لمادة الزنك (%25,50,75). الخصائص التركيبية والبصرية تم تحليلها باستخدام حيود الاشعة السينية ومطياف الاشعة المرئية – فوق البنفسجية. واظهرت نتائج حيود الاشعة السينية أن الاغشية الرقيقة ذات طبيعة متعددة التبلوروبتركيب الوجه المركزي المكعب. وبينت نتائج النفاذية البصرية بأن اغشية اوكسيد الكادميوم زنك ذات نفاذية عالية اكبر من 80% للمنطقة المرئية. وقد وجدنا عند زيادة تركيز اضافة الزنك ان فجوة الطاقة تزداد من (2.49 الى 2.9 الكترون فولت).


Article
Preparation Thin Filmsfrom SnS by successive ionic layer adsorption and reaction (SILAR) MethodandStudying Optical and Structural
تحضيراغشية رقيقة لكبريتيد القصدير بطريقة الغطس المتعاقب للطبقات الايونية ودراسة الخواص البصرية والتركيبة لها

Author: Afrah.AbdulHussain.Jabor افراح عبد الحسين جبر
Journal: Journal of College of Education مجلة كلية التربية ISSN: 18120380 Year: 2015 Issue: 5 Pages: 295-302
Publisher: Al-Mustansyriah University الجامعة المستنصرية

Loading...
Loading...
Abstract

SnS thin films have been deposited by Successive ionic layer adsorption and reaction (SILAR) methodat room temperature. The structural, of the film are determined by using X-ray diffraction (XRD)Measurement and optical propertiesMeasurement by using UV-Vsi spectrophotometer.The preparation of tin sulfide thin films of 0.3µm thickness were grown on glass substrates by SILAR method using SnSO4 and Na2S at different concentrations0.3M and 0.6 M. Polycrystalline structure of films are shown by XRD.

الخلاصةرسبت اغشية رقيق لكيريتيد القصدير بطريقة الغطس الايوني المتعاقب عند درجة حرارة الغرفة ثم درست الخواص التركيبية والبصرية للأغشية من خلال حساب حيود الاشعة السينية والبصرية باستخدام مطياف الاشعة الفوق البنفسجية والمرئية.تم انماء الاغشية على قواعد زجاجية وبسمك0,3مايكرومتر بطريقة الغطس المتعاقب للطبقات ا لايونية باستخدام كبريتات القصدير وكبريتيد الصوديوم وبتراكيزمختلفة (0.3 ,0,6) مولاري.ظهر التركيب متعدد التبلور للاغشية من خلال فحوصات حيود الاشعة السينية


Article
Effect Adding PVA Polymer on Structural and Optical Properties of TiO2 Thin Films

Authors: Arwa Fadil Saleh --- Ahmed Mousa Jaffar --- Najim A. Samoom --- Marwa Wailed Mahmmod
Journal: Al-Nahrain Journal of Science مجلة النهرين للعلوم ISSN: (print)26635453,(online)26635461 Year: 2014 Volume: 17 Issue: 2 Pages: 116-121
Publisher: Al-Nahrain University جامعة النهرين

Loading...
Loading...
Abstract

Thin films of titanium dioxide TiO2 pure and TiO2:PVA polymer were prepared using chemical spray pyrolysis technique on glass substrate preheated at (350 oC) for TiO2 pure, and at (160 oC) for TiO2:PVA. with spray rate 3sec./1min, and thickness (250nm). The investigation of (XRD) indicates that structural of TiO2 pure and TiO2: PVA thin films they are polycrystalline and XRD investigation is anatase titanium dioxide, intensity of >101< is more than the intensity of <004 >, <200< and >105< for TiO2 and TiO2:PVA thin films. The optical properties measurement explain the effect of adding PVA on Transmittance, absorptance, refractive index, absorption coefficient and electronic transitions of prepared thin films. and their results observed that filling of PVA caused increase in optical properties generally.

حُضرت أغشية ثناني أوكسيد التيتانيوم الرقيقة النقية TiO2 و المشوبة بالبوليمر TiO2:PVA بأستعمال تقنية التحلل الكيميائي الحراري على قواعد زجاجية مسخنة، بدرجة حرارة (350 oC) لتحضير أغشية ثناني أوكسيد التيتانيوم الرقيقة النقية TiO2، و بدرجة حرارة oC 160 لتحضير الاغشية المشوبة بالبوليمر TiO2:PVA بزمن رش 3 ثواني لكل دقيقة، و بسُمك 250 نانوميتر. فحوصات (XRD) بينت ان التركيب أغشية TiO2 النقية و المشوبة بالبوليمـر TiO2:PVA بأنهـا متعـددة التبلـور polycrystalline نوع anatase و ان شدة <101> أكبر نسبياً من <105>, <200>,<004> لكلا الغشائين النقي و المشوب بالبوليمر. كذلك تمت دراسة الخصائص البصرية للأغشية TiO2 النقية و المشوبة بالبوليمر TiO2:PVA حيث تم حساب الثوابت البصرية قبل و بعد إضافة البوليمر PVA كالنفاذية، الامتصاصية، معامل الانكسار، معامل الامتصاص، الانتقالات الالكترونية المباشرة المسموحة و الممنوعة، حيث بينت النتائج أن أضافة البوليمر PVA أثـرت بصورة واضحة في زيادة الثوابت البصرية عموماً لأنه سبب في ربط الاواصر بين الذرات و ذلك ادى الى زيادة الخصائص البصرية و التركيبية أيضاً.


Article
Antibacterial Activity of Boehmite Nanoparticles Synthesized by Arc Discharge in Deionized Water Technique

Author: Halah H. Rashed
Journal: Al-Nahrain Journal of Science مجلة النهرين للعلوم ISSN: (print)26635453,(online)26635461 Year: 2017 Volume: 20 Issue: 1 Pages: 58-65
Publisher: Al-Nahrain University جامعة النهرين

Loading...
Loading...
Abstract

In this work, boehmite AlO(OH) nanoparticles were synthesized by arc discharge technique. The structural, surface morphology and optical properties were characterized by X-Ray Diffraction (XRD), Fourier transforms infrared spectroscopy (FTIR), Atomic Force Microscope (AFM) and Ultraviolet-Visible-Near In far Red spectrophotometer respectively. XRD results show pure orthorhombic crystalline structure of gamma-AlO(OH). FTIR absorption spectrum shows that the boehmite nps have the octahedron region which extends from (400–800 cm-1) corresponding to the vibrational frequencies of Al–O bonding. The AFM shows that boehmite NPs are spherical in shape and the average diameter is around 89 nm. Finally the optical properties results show that the boehmite nps have absorption peak at 210 nm and an optical band gap of 4.1 eV.Boehmite nps was examined susceptibility to effect on the different types of bacteria, Escherichia coli (Gram-negative) and Staphylococcus aurous (Gram-positive) strains bacteria.Boehmite NPs showed excellent antibacterial activity against two types of bacteria. Also, Staphylococcus aurous exhibited the highest sensitivity to boehmite NPs while Escherichia coli were the least sensitive. [DOI: 10.22401/JNUS.20.1.08]


Article
Effect of Film thickness on Optical and Structural Properties of CdS Thin Films prepared by spray pyrolysis
تأثیر السمك على الخصائص التركیبیة والبصریة لأغشیة Cds الرقیقة المحضرة بطریقة التحلل الكیمیائي الحراري

Author: Mehdi H. Diwan مھدي حاتم دیوان
Journal: Diyala Journal For Pure Science مجلة ديالى للعلوم الصرفة ISSN: 83732222 25189255 Year: 2014 Volume: 10 Issue: 2 - part 2 Pages: 158-171
Publisher: Diyala University جامعة ديالى

Loading...
Loading...
Abstract

Cadmium sulphide ( CdS ) thin films were prepared by the chemical Spray Pyrolysis technique on glass substrates at 400°C. The analysis of x-ray diffraction spectra XRD , patterns indicated the presence of single-phase hexagonal CdS which confirmed through the atomic force micrographs (AFM) images. The structural parameters such as interplannar distance (d), lattice constant (a), grain size (D), and micro strain have been evaluated, The crystal growth became stronger and more oriented as seen in the x-ray diffraction spectra and grain size became larger with increasing in the thickness. The optical properties have been studied in the range (300-900)nm. It is observed that the direct band gap energy is inversely depended on film thickness from (2.36–2.34) eV.

حضرت أغشية كبريتيد الكادميوم بطريقة التحلل الكيميائي الحراري على قواعد زجاجية وبدرجة حرارة °C 400 .أوضحت نتائج فحوصات حيود الأشعة السينية إن الأغشية المحضرة ذات تركيب متعدد التبلور ونوعها أحادي الطور السداسي وتم تأكيد ذلك من خلال صور مجهر القوة الذرية المتغيرات التركيبية مثل المسافة بين السطوح البلورية (d), ثابت الشبيكة (a), حجم الحبيبات (D) تم دراستها. وأظهرت نتائج فحوصات حيود الأشعة السينية إن حجم الحبيبات يصبح اكبر بزيادة سمك الأغشية , الخصائص البصرية درست في مدى (300-900)nm وأوضحت إن فجوة الطاقة المباشرة المسموحة تتناسب عكسيا مع زيادة سمك الأغشية 2.36–2.34) eV ) .


Article
Study The Effect of Thickness on The Structural and Optical constant of CdSe Thin Films
دراسة تاثير السمك على الخواص التركيبية والثوابت البصرية لاغشية سيلينايد الكادميوم (CdSe)الرقيقة

Authors: T.H.Mahmoud طاهر حمد محمود --- B.K.Hassun بشرى كاظم حسون --- S.A.Make سمير عطا مكي
Journal: Journal of College of Education مجلة كلية التربية ISSN: 18120380 Year: 2017 Issue: 1 Pages: 249-264
Publisher: Al-Mustansyriah University الجامعة المستنصرية

Loading...
Loading...
Abstract

In this research , pure (CdSe) thin films with a different thickness ( 300 , 500 ,700 ,900) ± 20 nm was deposited on glass substrate in room temperature ( 300K ) with deposition rate (0.7±0.01) nm /sec by thermal evaporation under vacuum technique , and then studies their structure and optical properties .The resultant of the structural analysis showed that all films with all thickness prepared were polycrystalline in nature and have hexagonal type structure with atomic growth in three crystal orientation which it [002] , [102] and [103] with Preferred orientation along [002] plane for all Prepared films.The optical analysis measurement showed that all prepared films have absorption coefficient with a value larger than (∝ > 〖10〗^4 〖cm〗^(-1)) and this value was increased when increasing the film thickness especially in the visible range of electromagnetic spectrum , the optical energy gap was founded in the range ( 1.70 -1.72 ) eV.

تم في هذا البحث ترسيب اغشية سيلينايد الكادميوم النقية بطريقـــة التبخير الحراري فــي الفراغ عـلى قواعد من الزجاج بــدرجة حـرارة الغرفــــــة ( 300k) وبسمــك مـختلف 20 nm±) 900 ،700 ، 500 ، 300 ) وبـمعـدل تــرسيب sec / 0.7nm ووجد بـان الاغشيـة النـاتجة كـانت ذات جـودة عالية مــن حيــث تجانس الغشاء والتصاقيته بالارضيات الزجاجية، ودرسـت خواصها التركيبية والبصرية. اظهرت نتائـج الفحوصــات التركيبية بـان جميع الاغشيــة الرقيقة ,والمحضرة بسمك مختلف كانت متعددة التبلور ومـن النـوع السداسـي مع نمو ذري بثلاثة اتجاهات بلورية هـي [103] و[102] و[002] كان المميز والسائد منها في الاتجاه [002] وللنماذج المحضرة كافة .امـــا نتائج الفحوصات البصريــة فـقـد بــيـنت بـان مـعامـل الامتصـاص للاغـشية المحــضرة كـــان ذو قــيمة اكــبر من (〖cm〗^(-1) α >〖10〗^4 ) وان هـذه الـقيمة تـزداد بشكل عام بزيادة السمك لاسيما عند الطاقات الفوتونية الواطئة ، اما بالنسبة الى قيمة فجوة الطاقة البصرية فلقد كانت ضمن المدى eV(1.70-1.72) .


Article
Effect a Nd:YAG Laser Irradiation on The Optical And Structural Properties of Thin Film (CdO) Prepared by Chemical Spray Pyrolysis (CSP)Technique.
تأثير أشعة الليزرNd:YAG على الخصائص البصرية والتركيبية للأغشية الرقيقة (CdO) المحضرة بتقنية الرش الكيميائي الحراري

Loading...
Loading...
Abstract

To study the effect of Nd:YAG laser on the properties of structural and optical values of the energy gap of cadmium oxide (CdO) films, have been prepared using chemical spray pyrolysis and deposited on a glass substrate for concentrations(0.05, 0.1, 0.15)M at temperature (350°C) ,using 6 spray rate during (10) second for each spray . To study the optical properties of the film Prepared (CdO) before and after irradiation Nd:YAG laser with energy (200) mJ at different times (5,10,15)sec and at (1) meter far from the source using a(UV-Visible) spectrometer device and the extent of wavelengths, (300-1100) nm the results showed that the energy gap increased with increasing concentrations and was the ideal value when the concentration of (0.1)M, where the value of energy gap is (2.25)eV, but after laser irradiation redueced to (2)eV. The Atomic Force Microscope(AFM) has been used to study the structural properties of the composition and topography of the surface in two and three dimensions of the films prepared before and after irradiation, the results indicate that the surface rate roughness and the average root of the square less after irradiation, and it is observed ideal value for this property is at a concentration of (0.1)M. The crystalline structures and surface morphology of CdO thin film examined by XRD analysis. The result showed the films are polycrystalline for and crystalline granules prevailing levels of growth are at (220), (200), (111) the irradiation led to a slight change in the angle of diffraction in the lattice constants (a) and a decline in giving the peak tops.

لدراسة تأثير اشعة الليزر نديميوم - ياك Nd:YAG)) على الخواص التركيبية والبصرية وقيم فجوة الطاقة لغشاء أوكسيـد الكادميوم (CdO), تم تحضير اغشية رقيقة لأوكسيد الكادميوم (CdO) بأستـخدام طـريقـة الرش الكيميائي الحراري على ارضيات من الزجاج بتراكيز(0.05 ,0.15,0.1) مولاري وبدرجة (350°C ) وبمعدل (6) رشات خلال فترة زمنية (10) ثانية لكل رش. ولدراسة الخصائص البصرية للغشاء المحضر(CdO) قبل وبعد التشعيع بالليزر نديميوم- ياك Nd:YAG)) وبطاقة 200)mJ) بأزمان مختلفة (5,10,15) ثانية وعلى بعد (1) متر من المصدر أستخـدام جهـاز مطيـاف(UV-Visble) ولمدى الأطوال الموجية,(300-1100) nm اذ بينت النتائج أن فجوة الطاقة تزداد بزيادة التراكيز وكانت القيمة المثالية عند تركيز M(0.1) حيث كانت قيمتها eV(2.25), أما بعد التشعيع بالليزر تقل قيمتها الىeV 2)). وأستخدام جهاز المجهر القوة الذرية لدراسة الخصائص التركيبية ومعرفة التركيب النانوي وطوبوغرافية السطح في بعدين وثلاثة أبعاد للأغشية المحضرة قبل وبعد التشعيع بالليزر, اذ بيت النتائج أن معدل خشونة السطح ومتوسط الجذر التربيعي تقل بعد التشعيع, واتضح أن القيمة المثالية لهذه الخاصية هو عند تركيز 0.1)M). وأستخدم جهاز الاشعة السينية لمعرفة طبيعة تبلورالاغشية, اذ بينت نتائج الفحص ان تركيب الغشاء المحضر(CdO) هو تركيب متعدد التبلور وذلك لوجود أكثر من قمة وذات تركيب سداسي, وأن نمو الحبيبات البلورية السائدة للمستويات هي عند الاتجاهات (220),(200) , ,(111) واالتشعيع بالليزرادى الى حدوث تغيرات طفيفة في زوايا الحيود وفي ثابت الشبيكة (a) وهبوط في قمم منحي الذروة.

Listing 1 - 8 of 8
Sort by
Narrow your search

Resource type

article (8)


Language

English (6)

Arabic (1)

Arabic and English (1)


Year
From To Submit

2017 (2)

2016 (1)

2015 (2)

2014 (2)