Abstract Study of preparation involve the examination of the effects of operating variables on mechanical properties of polylactic acid /low density polyethylene (PLA/LDPE)/clay nanocomposites including tensile strength, modulus, and elongation at break. Thermal stability of these nanocomposites that’s investigated. Montmorillonite clay with alkyl ammonium ion of hexadecyl trimethylammonium bromide (CTAB) was examined. Among the parameters studied, PLA/ LDPE nanocomposites showed larger improvements in mechanical properties compared to PLA/ LDPE blend due to higher shear forces exerted by polymer blend matrix on clay aggregates during polymer-clay mixing. The original MMT with Na+ cation results in weak improvements in mechanical properties compared to organoclays. It was observed that the tensile strength, modulus, and elongation at break of the nanocomposite samples can be optimized with 4% of clay loading. The morphology and chemical structure of the optimum sample were examined by X-ray diffraction and FT-IR spectroscopy, respectively.

الخلاصةتتناول هذا البحث تحضير ودراسة تاثير المتغيرات على الخواص الميكانيكية للكوبوليمرالمتكون من حامض البولي لاكتيك / البولي اثيلين منخفض الكثافة (PLA / LDPE) مع الطين المعدل (organoclay) بطريقة النانوكومبوزت وتشمل هذه الخواص قوة الشد والمرونه واستطالة عند الكسر.ايضا تم دراسة الثباتية الحرارية للكومبوليمر بعد انتاجه بطريقة النانو . تم مفاعلة وفحص الطين من نوع مونتمورينوليت مع أيون هكساديسايل ثلاثي مثيل الامونيوم trimethylammonium hexadecyl (CTAB)لانتاج الايون (organoclay) الذي يعمل بطريقة النانو. اضهرت النتائج على دراسة PLA/LDPE نانوكومبوزت ان هنالك تحسن كبير في الخواص الميكانيكية والحرارية كما ظهر في فحص TGA والتنسايل والمرونه مقارنة بمزيج PLA/LDPE لوحده حيث ان الطين المعدل(organoclay) المضاف حسن من قوة تحمل البوليمرللحرارة والشد . كما تمت ملاحظة ان قوة الشد التنسايل والاستطارة قد ازدادت بوجود الطين المعدل المضاف بمعدل 4% فيما قلت هذه الخواص عند زيادة النسبة عن 4% . ايضا تم فحص التركيب الكيميائي والمورفولوجي للناتج للعينة الامثل المضاف لها 4% من الطين المعدل بواسطة FTIR و XRD ايضا تم اخذ صور للناتج لاضهار النانو بواسطة SEM و TEM .


Article
Properties characterization of plasticized polylactic acid /Biochar (bio carbon) nano-composites for antistatic packaging
تشخيص مواصفات المتراكب لملدن البولي لاكتك اسد مع الكاربون الحيوي في الاغلفه ضد الكهربائيه الساكنه

Authors: Saif Mohammed Jasim سيف محمد جاسم --- Nadia Abbas Ali نادية عباس علي
Journal: Iraqi Journal of Physics المجلة العراقية للفيزياء ISSN: 20704003 Year: 2019 Volume: 17 Issue: 42 Pages: 13-26
Publisher: Baghdad University جامعة بغداد

Loading...
Loading...
Abstract

A new type of light-weight nanocarbon prepared by the spray-drying method to obtain particle size of 21.7 nm based on the polylactic acid biodegradable film in antistatic packaging. Biocarbon (biochar) is the carbon derived from plants, and soils to naturally absorb and store carbon dioxide from the atmosphere because it is renewability. Therefore it has been used to reinforce biodegradable polylactic acid (PLA) to obtain 100 % recyclable material. Plasticizer thymol of polylactic acid and biochar (biocarbon) were used as composites were prepared by a solution casting method with (0.5-10) wt% biochar. The films were characterized using FTIR, electrical conductivity, mechanical properties, contact angle and color and brightness were studied. Results showed that electrical conductivity of increased with increased biochar making the composite less resistive and suitable for use as antistatic packaging for the transportation and storage of electronic components. Mechanical tests showed reduced tensile strength and tensile modulus but increased in elongation. Also Tear Resistance and Hardness decreased because used thymol as plasticizers at PLA/thymol (95/5) and films composites change from brittle to ductile. The results of the contact angle of pure PLA is 83◦ means hydrophobic materials and decreased to 54◦ at PLA/thymol/biochar 10% to obtain hydrophilic materials which is able to dissipate or promote the decay of static electricity and improve the processability of the electronic device. Optical properties such as color and brightness showed decreased but suitable for antistatic packaging and became opacity at 10% biochar.

تم تحضير نوع جديد من الكاربون النانوي بطريقه التجفيف – الرش وتم الحصول على الجسيمات بحجم حبيبي 21.7 نانو متر استخدم مع البوليمر الحيوي المتحلل البولي لاكتك اسد في تطبيق الاغلفه ضد الكهرباء الساكنه. الكاربون الحيوي المستخدم تم الحصول عليه من النبات والاشجار الذي يمتص غاز ثاني اوكسيد الكاربون القابل للتجديد. تم استخدامه كمواد تقويه في البولي لاكتك اسد الحيوي للحصول على متراكب متحلل بنسبه 100%.تم استخدام الملدن الثايمول مع المتراكب بولي لاكتك اسد والكاربون الحيوي لتحضير المتراكب بطريقه الصب بنسب مئويه وزنيه تراوحت بين (0.5-10) wt%, تم التشخيص باستخدام تحويلات فورير للاشعه تحت الحمراء والتوصيليه الكهربائيه والخواص الميكانيكيه وزاويه التماس واللون وشده السطوع. اظهرت النتائج بان التوصيليه الكهربايه تزداد مع زياده نسبه الكاربون الحيوي والتي تجعل المتراكب ذات فائدة ومناسب لاستخدامه في التغليف المضاد للكهرباء. اما الفحوصات الميكانيكيه اظهرت انخفاض في معدل الشد ومعامل الشد مع زياده في معدل الاستطاله ومقاومه التمزق والصلادة بسبب استخدام الثايمول كملدن بنسبه 5% وبذلك تتغير الماده من السلوم الهش الى اللدن. نتائج زاويه التماس للبوليمر بولي لاكتك اسد هي 83◦ والتي تبين بان الماده كاره للماء وانخفضت في المتراكب لتصل الى ◦54 لتتحول الى السلوم المحب للماء الذي يعمل على تقليل من الكهرباء والشحنات المتولده على السطح وتحسين قابليه الغلاف. نتائج فحص اللون والسطوع انخفضت بشكل قليل ولكنها مناسبه للتغليف ضد الكهربائية الساكنه وازدات عتوميه عند النسبه 10 % من الكاربون الحيوي.

Listing 1 - 2 of 2
Sort by
Narrow your search

Resource type

article (2)


Language

English (2)


Year
From To Submit

2019 (1)

2013 (1)